Preferential corrosion of Fe element in NiFe_2O_4-10NiO based ceramic for aluminum electrolysis

Xiao Hanning

Open full text

Abstract

The electrolysis corrosion performance of NiFe2O4-10NiO based ceramic was investigated in high temperature melt of 78.07% Na3AlF6-9.5%AlF3-5.0%CaF2-7.43%Al2O3.The results showed that Fe/Ni atomic ratio in NiFe2O4 and NiO phase after sintered is 2.211-2.89 and 0.136-0.34,respectively,but Fe/Ni atomic ratio in NiFe2O4 and NiO phase after electrolysis is 2.07-2.335 and 0.120-0.195,respectively.So the Fe/Ni atomic ratio in NiFe2O4 and NiO phase decreased in some extent and preferential corrosion of Fe element happened in the process of aluminum electrolysis.Possibly the synergism of chemical corrosion and electrochemical corrosion result in the preferential corrosion dissolution of Fe element.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Bauxite Residue and Utilization · Metallurgy and Material Science · Molten salt chemistry and electrochemical processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.