High pressure and low-temperature sintering of AlN ceramics with La_2O_3 as a sintering aid
Source abstract
Abstract
Aluminum nitride ceramics with La2O3 as a sintering aid were fabricated under high pressure(5.0GPa) at a low temperature(1300-1800℃) in a cubic anvil high-pressure and high-temperature apparatus(China type).The characterization of the sintered bodies was determined by XRD,SEM and Micro-Raman spectroscopy.The results showed the method could lower the sintering temperature and shorten the sintering time effectively.Under high pressure of 5.0GPa,the lowest sintering temperature was 1300℃,which was above 300℃ lower than that for conventional liquid-phase sintering.The lattice parameters of the specimens sintered at high pressure were found to decrease by about 0.09% than that of the AlN powder and residual compressive stress was found,while hexagonal lattice of AlN was not changed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.