Prepared porous β-TCP Bioceramic by amylum pore-forming method
Source abstract
Abstract
Porous β-TCP bioceramic was made by calcined amylum in high temperature,which use amylum nature of irreversible expansion after amylum hydrophilic and adhesive action after expansion.Solid-to-liquid ratio was controlled in the range of 1.7-2.5 which is used for the intensity of body;β-TCP powders and sintered porous body were tested by XRD.After analysis,we can see that porous body's CPS are sharper than powders's.it shows that crystal grain grow very well;the results of SEM indicate that the material take on macropore-micropore structure.Among the pore,there are connectivity in three dimensions,the aperture of macropore is about 100-500μm,and the minipore is about 3-50μm,which are advantage of tissue growing and degradation reaction of material;mechanical behaviour measure indicates that compression strength is in the rang of 3-7MPa,porousity is about 40%-80% when amylum addition are in the range of 5%-20%.So we can see the material basically meet the requirement biology,it is a well bone recovery material.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Dental Implant Techniques and Outcomes · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.