Hydrogen storage of quasicrystalline Ti_(38)Zr_(45)Ni_(17)and after V alloying

MA Ren-tao

Open full text

Abstract

This paper investigates hydrogen absorption and desorption properties of quasicrystalline Ti_(38)Zr_(45)Ni_(17) and V-alloyed(Ti_(0.38)Zr_(0.45)Ni_(0.17))_(100-x)V_x(x=5%,10%,30%,40%,60at%).The composition design for the qua- sicrystal is uses the cluster line approach,where two cluster lines Zr_8Ni3-Ti and Ti_9Ni_4-Zr intersect at the ter- nary quasicrystal composition Ti_(38)Zr_(45)Ni_(17)in the Ti-Zr-Ni system.The alloy rods with a diameter of 3mm are prepared by copper mould suction-casting method.The experimental results indicate that the Ti_(38)Zr_(45)Ni_(17)quasic- rystal can absorb 0.9wt% of hydrogen at the first time at 303K,while the first-time maximum hydrogen content at 573K reaches 2.38wt%.The hydrogen-absorbing process is finished in a very short time,with the release of a large amount of heat which can even sinter the powder sample.The quasicrystal structure completely convert to hydrid after hydrogen absorption.5%-30at% V alloying of the ternary quasicrystal composition enhances the first-time hydrogen absorption capacity with the maximum reaching 2.96wt% at 573K.The solid solution alloy (Ti_(0.38)Zr_(0.45)Ni_(0.17))_(40)V_(60)absorbs hydrogen at room-temperature with a capacity of 3.2wt% hydrogen.Both the quasicrystalline and its V alloying quaternary alloy convert into hydrid after hydrogen absorption,which causes the hydrogen releases are difficult.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Quasicrystal Structures and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.