Fabrication and low temperature sintering of GDC thin film
Source abstract
Abstract
Gadolinia doped ceria(GDC) nano-powder was synthesized through a homogeneous precipitation process,using hexamethylenetetramine as the precipitator.XRD revealed that the as-synthesized powder already had a cubic fluorite structure of ceria,and BET revealed that the GDC powder had a surface area of 68.3m2/g and an average grain size of about 12 nanometers.Sintering behaviors of the GDC powder were studied via non-isothermal experiments.It demonstrated that the powder exhibited high sintering activity,where GDC green films prepared via dip coating using the slurry directly formed by the homogeneous precipitation process can be sintered to nearly full density at 1300℃,as revealed by the Field Emission SEM investigations.The thickness of the sintered GDC film after one coating-sintering cycle was 3μm and it can be controlled through adjusting the GDC concentration in the slurry and repeating the coating-sintering cycle.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Catalytic Processes in Materials Science · Advancements in Solid Oxide Fuel Cells · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.