Orthogonal experiment-aided analysis the leading factors of Bi_(0.5)Na_(0.5)TiO_3 powders prepared by sol-gel method
Source abstract
Abstract
Bismuth sodium titanate [Bi0.5Na0.5TiO3,BNT] fine powders can be prepared using tetrabutyl titanate,bismuth nitrate pentahydrate and sodium acetate anhydrous as starting materials by sol-gel method.The structure characteristics and microstructure of the synthesized powders were analyzed by XRD and TEM.Applying orthogonal experiment method,the influence of reaction temperature,pH and water volume on the grain size of final BNT powders were analyzed.It was founded that,the primary and secondary sequence affecting the grain sizes of the BNT powders is:water volumepHreaction temperature.The results show that when the reaction temperature is 60℃,value of pH is 4.5 and the water volume is 7.2mL,the grain sizes of the powders is about 200-350nm.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicone and Siloxane Chemistry · BIM and Construction Integration · Spacecraft Design and Technology
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.