article·1999-01-01Open access

Influence of Doping on the Structure of Iron-oxide Nanocrystalline Phase

Wang Yuan‐sheng

Open full text

Abstract

The grain size and fine structure Of Sb doped α- Fe2O3 nanocrystalline phase obtained by sol-gel process have been studied withX-ray diffraction, transmission electron microscopy and Mossbauer spectrometer. The results show that, before doping, the grain size of α-Fe2O3 formed through crystallization Of Fe(OH)3 amorphous dry gel is rather coarse, atter Sb dOPing, some of the Sb atoms Participate inthe formation Of FeSbO4, while others enter the α- Fe2O3 lattice and form the interstitial solid solution. They seem to be mainly segregatednear the Surface of the grains and form the barrier for atomic diffusion, thus take the role of restraining the grain growth during heating.When heat treated at high temperature, the Sb solute stoms separate out from α- Fe2O3 phase and enable the rapid growth of the grains.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Iron oxide chemistry and applications · Minerals Flotation and Separation Techniques · Metal Extraction and Bioleaching

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.