article·2001-01-01Open access

Thermodynamic Analyses on (111) and (100) Facets Orientation Growth of CVD Diamond Film

Zhijie Liu

Open full text

Abstract

CH3 and C2H2 are the dominant growth precursors during chemical vapor deposition diamond process. The ratio of C2H2 to CH3 concentration ([C2H2]/[CH3]) will affect the growth orientation of diamond film. In this paper [C2H2]/[CH3] as a function of substrate temperature is calculated under 4kPa pressure according to a non-equilibrium thermodynamic coupling model reported previously. Diamond (111) and (100) facets growth is discussed with the ratio of C2H2 to CH3 concentration under various substrate temperatures and CH4 concentrations. With the increase of substrate temperature or CH4 concentration, [C2H2 ]/[CH3] will rises. So the growth rate of diamond (111) facets controlled by C2H2 concentration is higher than that of diamond (100) facets controlled by CH3, and thus (100) facets appear. When oxygen is added to the gas phase for CVD diamond,[C2H2 ]/[CH3]will reduce, thus the growth of diamond film with (111) facets will be benefited. These results are well consistent with many experiments reported by other researchers.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Force Microscopy Techniques and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References