Research on magnetic performance of Nd_(13)Fe_(80.1-x)Ti_xB_(6.5)Zr_(0.1)Cu_(0.3) permanent magnetic alloy
Source abstract
Abstract
HDDR(hydrogenation-disproportionation-desorption-recombination)process is an effective means by which the anisotropy Nd2Fe14B-base magnetic powder can be made.In this text,the influence rules of d-HDDR process and the additive element Ti on the magnetic performance of Nd13Fe80.1-xTixB6.5Zr0.1Cu0.3(x=0,1.0,2.0)alloy are studied.The results indicate that:In the d-HDDR process,the hydrogen press and disproportionation time is the key to cause materials to produce anisotropy;Element Ti enhances the coercive force of NdFeB alloy notably,it has two functions:on the one hand,forming lower temperature fusant on the grain boundaries,restraining grain growth,improving the structure of rich in Nd phase and making the rich in Nd phase distribute equably along the boundaries;In addition,element Ti makes the NdFeB grain boundaries smooth and clear,enhances the main phase grain surface anisotropy,makes back magnetic domain nucleate difficultly,thereby,the coercive force is enhanced,the best adding dosage of element Ti is 1.0at%.The best performances of the 2# alloy Nd13Fe79.1Ti1.0B6.5Zr0.1Cu0.3 treated by d-HDDR process are as follows:Br=1.39T;iHc=1006kA/m;(BH)max=169.66kJ/m3;DOA=0.797.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic Properties and Applications · Electric Motor Design and Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.