Nano-sized Y_2O_3 powder preparaed by modified precipitation method
Source abstract
Abstract
Y_2O_3 precursor was synthesized via a modified precipitation method with Y(NO_3)_3 and NH_4HCO_3 as the raw material,and a proper amount of surfactant(polyvinyl alcohol) and(NH_4)_2SO_4.Then nano-sized Y_2O_3 powder was produced through calcining precursor at different temperatures.The calcined powder was measured by means of XRD,TEM and TG-DTA.The results are shown that,the Y_2O_3 particle calcined at 900℃ for 1.5h possesses sphere-like shape,uniform size(7nm),excellent dispersity and flowability.