Formation of Fe_(60)Co_8Zr_(10)Mo_5W_2B_(15) bulk amorphous alloy and influences of subsequent heat treatment on the properties
Source abstract
Abstract
Bulk amorphous rods,Fe_(60)Co_8Zr_(10)Mo_5W_2B_(15) and Fe_(60)Co_8Zr_8Mo_5W_2Nb_2B_(15),with a diameter of 2mm have been obtained by using copper mould suction cast.For Fe_(60)Co_8Zr_(10)Mo_5W_2B_(15),the structure,thermal stability,and the micro-hardness and compression strength before and after annealed,have been investigated by X-ray diffraction,differential scanning calorimetry,micro-hardness and compression tests.A small addition of niobium replacing with zirconium is not beneficial for improving glass-forming ability.Fe_(60)Co_8Zr_(10)Mo_5W_2B_(15) bulk amorphous alloy shows microhardness about 1343HV0.2 and compression strength about 972.6MPa.As annealed below the onset of crystallization temperature,the hardness decreases slightly.However annealed above the peak of crystallization temperature,the hardness will first increase and then gradually decline with the elongation of annealing time.Furthermore,annealed for the same period of time,the microhardness will increase with the rise of annealing temperature,while the compression strength will apparently decrease.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metallic Glasses and Amorphous Alloys · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.