article·2005-11-20Open access

Fabrication of TiAl nano-alloy by mechanical activation-spark plasma sintering process in situ

Zhiwei Wang, Yu-Xiang Shi

Open full text

Abstract

Powder of (Ti-50at%Al-10wt%Al2O3 was get through ball milling mechanical activation (MA), and then sintered and concurrently consolidated by using spark plasma sintering (SPS) process. TiAl-Al2O3 bulk nano-material was fabricated using the method of mechanical activation-spark plasma sintering (MA-SPS) in situ. The original and ball milled (Ti-50at%Al)-10wt%Al2O3 showed similar X-ray diffraction profiles. After MA, the crystal sizes of nano-powder are less than 25nm. Al2O3 has effect of mechanical activation, while makes crystal fine and accelerates nano-process. The nano-powder was sintered into TiAl alloy on a temperature lower than 800℃, and for a sintering time less than 5mm. The microstructure of TiAl alloy contains gamma TiAl and alpha-2 Ti3Al phase. Through SPS in situ, the final nano-material has dual-phase (λ+α2), and its density is 3.73g/cm^3. The crystal sizes of dual-phase are less than l30nm.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · nanoparticles nucleation surface interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.