Study on the function mechanism of C_3H_8O_3 on ceramic coating formed of ZAlSi12Cu2Mg1 by MAO
Source abstract
Abstract
In the present study,the micro-arc oxidation coatings of ZAlSi12Cu2Mg1 are obtained at 480V forward voltage,130V reverse voltage and a electrolyte containing 8g/L Na2SiO3,2g/L NaOH,2g/L Na2WO4 and 2g/L Na2EDTA.The influences of content of Glycerin on the arc starting voltage,thicknesses and microhardness of coatings,phase distribution and morphology of coatings were analyzed respectively.The results show that less rough and higher microhardness coatings are formed from an electrolyte with addition of C3H8O3.With the content of C3H8O3 ascending from 0 to 10mL/L,the mean diameter of colloidal particle descends from 10530.6 to 2615.8nm,the thickness of coatings rises gradually from 63 to 156μm,the dimension of the ceramic grains and the proportion of compact layer increase,and the microhardness of coatings reach HV894.But as the content of C3H8O3 excess 10mL/L,arc starting voltage ascends 408V.The result indicates by XRD that the coatings formed from an electrolyte with addition of C3H8O3 were composed of mullite,α-Al2O3,γ-Al2O3,WO3 and SiO2.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References