Electrochemical preparation of SrWO_4 film and its photoluminescence properties at room temperature
Source abstract
Abstract
Crystallized SrWO_4 thin films with scheelite-structure were prepared directly on tungsten substrate by using constant current electrochemical method at room temperature.The parameters of the electrochemical reaction were controlled as:current density was 1mA/cm~2;the pH value of electrolytes was 12.5 and the duration of electrochemical treatment was 1.5h.The as-grown thin films were characterized by using XRD, SEM and XPS respectively.At room temperature,the photoluminescence properties of as-grown SrWO_4 thin films were measured for the first time,the test results show that SrWO_4 thin film emits a stronger spectrum in about 400nm with a couple of serial weaker spectra in the range of 450~580nm when it was excited by 325nm laser.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Gas Sensing Nanomaterials and Sensors · Analytical Chemistry and Sensors · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.