Preparation of high density Ni_(0.8)Co_(0.2)(OH)_2 used as precursor for cathode of lithium battery
Source abstract
Abstract
Precursor-Ni0.8Co0.2(OH)2 with high tapping density was prepared by second stage drying method.The effects of reactants concentration,reaction temperature,cake moisture,drying method,etc.on the tapping density of Ni0.8Co0.2(OH)2 were discussed.The optimum process parameters of preparing the fine Ni0.8Co0.2(OH)2 were that the concentration of NiSO4 is 1.66mol/L,the reaction temperature was 50℃,the cake moisture was kept properly.The tap density of the prepared non-spherical Ni0.8Co0.2(OH)2 powder reached 2.23g/cm3.XRD revealed that the material was β-Ni0.8Co0.2(OH)2 and had better structure on the whole.LiNi0.8Co0.2O2 powders was synthesized by sintering the Precursor-Ni0.8Co0.2(OH)2 with high tapping density and LiOH·H2O,and electrochemical property tests testified that LiNi0.8Co0.2O2 had good electrochemical performance.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Transition Metal Oxide Nanomaterials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.