Dehydrogenation kinetics of hydrogen storage material 67Mg29C3Ni1Al

Yang Min-jian

Open full text

Abstract

The hydrogen storage material 67Mg29C3Ni1Al was prepared by reactive ball milling using the mixed powder of coal-based crystallitic carbon,magnesium,nickel,and aluminum under the hydrogen pressure of 1MPa for 3h.The dehydrogenation test results showed that the dehydrogenation capacity was larger and the dehydrogenation speed was quicker with the increase of temperature.The apparent dehydrogenation reaction was the first order reaction which was obtained by data fitting.By means of Arrhenius equation,the apparent activation energy of 67Mg29C3Ni1Al is calculated and the value is(138.0±6)kJ/mol within the limits of 300-350℃.Compared to the hydrogen storage material 70Mg30C and MgH2,the crystallitic carbon and the catalysts of Ni and Al cut down the dehydrogenation time,increased the dehydrogenation capacity of hydrogen storage material,and reduced its apparent activation energy.And the dehydrogenation kinetics performance was improved.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen Storage and Materials · Hybrid Renewable Energy Systems · Ammonia Synthesis and Nitrogen Reduction

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.