Preparation of Y_2O_3∶Eu~(3+) red phosphor by firing assisted with(Na_2CO_3+S+NaCl) compound molten salt
Source abstract
Abstract
The precursor of Y2(C2O4)3∶Eu3+ was prepared by homogeneous precipitation-molten salts method.The molten salt,such as Na2CO3,S,NaCl or their combination is assistant of preparing Y2O3∶Eu3+ red phosphor in the process of sintering precursor at 1000-1300℃ for 2h.The effect of molten salt on particle size and luminescent intensity is also studied.The experimental results show that the compound molten salt is in favor of improving the luminescent intensity of Y2O3∶Eu3+.The intensity of the emission peak is 36% higher than that of the phosphor doped without molten salt and 11% higher than the corresponding commercial phosphor when the sintering temperature is 1300℃.At the same time,the particle size of Y2O3∶Eu3+ phosphor is controlled effectively by the molten salt.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.