article·2004-01-01Open access

Preparation and property of Ca_2Co_2O_5 thermoelectric material by spark plasma sintering

LU Qin-meion

Open full text

Abstract

The precursor of Ca_2Co_2O_5 was prepared by coprecipitating method using stoichiometric amounts of Co(NO_3)_2·6H_2O, Ca(NO_3)_2·4H_2O, and NaOH as precipitation agent. After heat treatment, the precursor was sintered by SPS process. ICP, DTA-TG, XRD and SEM are used to determine the decomposition in the process of heat treatment and the formation of Ca_2Co_2O_5. In order to obtain stoichiometric precursor, the ICP results show the ended pH value was 13.2. The precursor was heat treated in the range of 700℃ to 800℃ for 2h, and then sintered by SPS. XRD patterns show that the pure phase Ca_2Co_2O_5 was produced when sintering temperature was 800℃, the pressure was 30MPa, and last for 5min. SEM shows that the microstructure of the production was plate-like about 1.4μm. The thermal conductivity decreases with increasing temperature up to 800℃.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Thermoelectric Materials and Devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.