Effect of sintering temperature on the macro-characteristics and microstructure of MgB2 superconductor

Xu Zheng

Open full text

Abstract

Mg powder and B powder with a ratio of 1.03∶2 were well mixed and pressed into pellets.Samples were sintered for 1h at 660,700,750,800,850 and 900℃,respectively,in a flow of high purity argon gas.X-ray diffractometer,scanning electron microscopy and the Archimedes method et al.were used to investigate the phase composition,the microstructure,the density and so on of MgB2 samples.It is revealed that the macro-characteristics and the microstructure of the MgB2 bulk,such as the content of the non-superconducting phase of Mg and MgBx(x=4,6 or 12),the volume expansion coefficient,the mass loss rate,the density and the size of MgB2 grain,changes with the sintering temperature increasing.The high content of MgB2,the small grain size and the high density,which is beneficial to the superconductivity,can be achieved in the MgB2 bulks synthesized between 750 and 850℃.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Superconductivity in MgB2 and Alloys · Boron and Carbon Nanomaterials Research · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.