Zinc oxalate powders were prepared through interfacial stripping precipitation method with P204 diluted by tetrachloride carbon as an extractant,and oxalic acid ethanol aqueous solution as a reextractant and precipitator.Zinc oxide powders were obtained by decomposing zinc oxalate powder at 450℃.The results showed that the P204 contents in the oil phase,oxalic acid,ethanol contents in the water phase and temperature had obviously influence on the size distribution of zinc oxide powders.ZnO powders with the average size of about 32nm was obtained under an optimum condition with P204 35%(v/v)in oil phase,H2C2O4 0.3 mol/L and ethanol 80%(v/v)in water phase,reaction temperature 20℃.The kinetics study of the photocatalytic oxidation about ZnO showed the optimum catalyst loadings was 0.4g/L。
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.