Effects of sintering temperature and pre-treatment on ultrafine cemented carbides prepared by spark plasma sintering
Source abstract
Abstract
The ultrafine WC-10Co cemented carbides were prepared by high-energy boll milling and spark plasma sintering(SPS) using sub-micron WC/micron Co as the raw powder.The SPS process,microstructure and properties of the sintered samples were investigated.The sample sintered at 1200℃ has better mechanical properties than that sintered at 1150℃,such as relative density of 98.6%,hardness of 94.0HRA,transverse rupture strength(TRS) of 1819MPa.The composite was pretreated before sintered,and the sample has better mechanical properties than the samples sintered with no pretreated composite,for example,relative density of 99.1%,TRS of 1937MPa sintered at 1150℃.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.