Improvement of the electrochemical properties of Zr-based hydride electrodes by ball milling Zr_7Ni_(10)
Source abstract
Abstract
To improve the electrochemical properties of the Zr0.5Ti0.5Mn0.7V0.2Co0.1Ni1.2 alloys,surfaced modifications of the alloy by ball milling with Zr7Ni10 alloy have been carried out.The effects of both ball milling time and content of Zr7Ni10 on the structure and electrochemical characteristics of the alloys have been investigated.The results show that after ball milling with 8wt% Zr7Ni10 for 1 h,the alloy still maintains crystalline and exhibits the discharge capacity 266mAh/g at the current of 50mAh/g after 9 cycles,which is higher 20% than that of the alloy without ball milling,and it preserves 85% of maximum discharge capacity at the current of 300mA/g.However,alloys turn to be amorphous gradually with ball milling time increasing,especially more than for 3h,and their discharge capacities decreased sharply.Most of the amorphous alloy has been recrystallized after heat treatment at 800℃ for 1h,but its discharge capacity only is 200mAh/g after 22 cycles.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nuclear Materials and Properties · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.