article·2011-01-01Open access

Preparation of Si_(80)Ge_(20)B_(0.6) alloy by spark plasma sintering and their thermoelectric properties

Fu Guo

Open full text

Abstract

Single-phase Si80Ge20B0.6 alloy bulks were prepared by high-energy ball milling followed by spark plasma sintering method.The thermoelectric properties were measured from 400 to 900K.The carriers were scattered by grain boundaries in the alloys prepared by powder metallurgy.The bulk specimens heated for a longer period of time during SPS had higher electrical conductivity.The thermal conductivity values for all specimens were between 2.7 and 4.5 W/(m·K).The figure of merit ZT of the holding for 9 min specimen reached 0.47 at 900K.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and interfaces · Silicon and Solar Cell Technologies · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.