Microstructure and performance of CrN/Ag coating prepared in 800℃ with different Ag contents
Source abstract
Abstract
CrN/Ag hard coatings are prepared by DC reactive magnetron sputtering at 800℃.With the aim of clarifying the effects of Ag conentent and heat treatment on the performance of the CrN/Ag hard coating,the coating microstructure,chemical compositions and hardness are characterized by XRD,SEM,and Vickers hardness tester.The results indicate that the Ag addition leads to the roughening of the coating surface and the change of the coating growth direction from(200) preferred orientation to random orientations.A small amount of Ag addition(7at%) can slightly improve the coating hardness,while the further increase of Ag addition(21at%) causes dramatic hardness decrease.Pure CrN coating exihibits high oxidation resistance after a heat treatment at 700℃ for 1h.With the increase of Ag addition,however,the coatings show more serious oxidation.Furethermore,21at% of Ag addition leads to pronounced Ag diffusion to the coating surface.The oxidation and Ag diffusion result in the decrease of the coating hardness after the heat treatment.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · GaN-based semiconductor devices and materials · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.