article·2006-01-01Open access

Microstructure and electrochemical characteristics of Ti_(0.17)Zr_(0.08)V_(0.34)Cu_(0.01)Cr_(0.1)Ni_(0.3)hydrogen storage alloy

Meiye Li

Open full text

Abstract

Microstructure and electrochemical properties of Ti_0.17Zr_0.08V_0.34Cu_0.01Cr_0.1Ni_0.3 hydrogen storage alloy have been investigated by using XRD,FESEM-EDS,ICP and EIS measurements.The result of XRD and FESEM-EDS analysis shows that the alloy is mainly composed of V-based solid solution phase with body-centered-cubic(BCC) structure and C14 Laves phase with hexagonal structure,V-based solid solution phase forms dendric with C14 Laves phase surrounding it.The alloy electrode has a good discharge capacity within a wide temperature region from 303~343K,and the discharge capacity is 316.5mAh/g at 343K.The discharge capacity of the alloy electrode is 278.2mAh/g and the charge retention is 87.0% after 100th cycles at 303K,which shows the alloy electrode has good cycle stability,but the HRD is lower than other alloys.The result of electrochemical impedance spectrometry(EIS) indicates that charge transfer resistance(R_T) is decrease with increasing temperature,while exchanging current density is increase with increasing temperature.The dissolution of V and Zr element to KOH electrolyte is seriously,which is perhaps a main factor to affect the discharge capacity.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen Storage and Materials · Hybrid Renewable Energy Systems · Metallurgical and Alloy Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References