Powder injection molding of 4J36 invar alloy
Source abstract
Abstract
With the carbonyl iron powder and nickel powder as raw materials and a multi-component wax-based polymer as binders,the process and properties of 4J36 Invar alloy fabricated by powder injection molding (PIM) were studied. The results showed that it was facilitate to obtain high-performance PIM 4J36 Invar alloy by improving the sintering temperature or using a suitable sintering atmosphere. Under optimizing the sintering conditions as the sintering temperature of 1350℃,sintering time of 120min,sintering atmosphere of hydrogen,the relative density of 4J36 Invar alloy reached 98.1% and its average thermal expansion coefficient from room temperature to 100℃ was only 0.97×10-6℃-1 which is better than that of traditional technique. The microstructure and X-ray diffraction result both showed that the Invar alloy presented with only a single stable austenitite phase (γ-phase).
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Injection Molding Process and Properties · Advanced materials and composites · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.