Preparation of LaGaO_3 based electrolyte for intermediate temperature SOFC
Source abstract
Abstract
The electrolyte La_(0.9)Sr_(0.1)Ga_(0.8)Mg_(0.2)O_(3-δ) was prepared by the method of solid state reaction and gel-combustion method respectively, X-ray diffraction was used to characterize the phase transition with the calcination temperature. The result showed that the single phase LSGM was formed at 1400℃ with 10h by gel-combustion method with particle size 150nm and phase LSGM was formed at 1500℃ with 24h by solid state reaction with particle size 1μm .
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Gas Sensing Nanomaterials and Sensors · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.