Study on sintering technique of NiFe_2O_4/SiC_w used as matrix of inert anodes

Yihan Liu

Open full text

Abstract

In order to improve deficiencies of NiFe_2O_4 spinel used as matrix of inert anode in aluminium electrolysis, NiFe_2O_4/SiCw were prepared by the solid state reaction for the first time. Microstructural changes were observed by scanning electronic microscope and phase was determined with X-ray detector. Effect of sintering temperature and times on density, porosity and microstructure were researched, and the reasons that caused the difference were discussed deeply. At the same time the thermodynamical compatibility of NiFe_2O_4 and SiC was proved under 1200℃ by DTA . The results showed that the microstructure was more homogeneous when the sintering temperature reached 1180℃ and the density attained their maximum about 6h sintering. The appropriate sintering technique of NiFe_2O_4/SiC_w composite materials selected 1180℃×6h.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Bauxite Residue and Utilization · Advancements in Battery Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.