article·2014-01-01Open access

Rolling process and texture evolution of 6.4wt% silicon steel with low iron loss and high magnetic induction

Qin Jin

Open full text

Abstract

6.4wt%Si high silicon steel sheets(0.23mm thick)with low iron loss and high magnetic induction were successfully produced by rolling process.The final magnetic properties along the rolling direction(RD) were:B8=1.474T,B50=1.714T;P10/50=0.30 W/kg,P15/50=0.88 W/kg.The texture evolution during rolling and annealing was investigated by means of X-ray diffraction and electron backscatter diffraction(EBSD).It was found that more Goss textures formed in the subsurface of hot rolled plates by using large hot rolling reduction,and then was inherited;the coarse grains in warm rolled plate were good for the formation of shear band during cold rolling;the high magnetic induction along the RD was achieved after decarburization annealing due to the formation of strong{210}〈001〉and Goss texture which mainly nucleated and grew within shear bands of the deformed{111}〈112〉grains;although some random orientation existed after final annealing, the magnetic induction was further improved due to the retention and enhancement of{310}〈001〉inηtexture. With the increasing of annealing temperature and annealing time,the grains of the high silicon steel sheet grew and the iron loss decreased significantly.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnetic Properties and Applications · Microstructure and Mechanical Properties of Steels · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References