Study on the shrinkage of foamed concrete with shrinkage-reducing admixtures
Source abstract
Abstract
To prevent cracking caused by shrinkage,pore structure,drying shrinkage and autogenous shrinkage of foamed concrete with SRA( S1 and S2),were studied by testing drying shrinkage and autogenous shrinkage and analyzed by MIP,BET,XRD,when W /C were 0. 33 and 0. 50. The result showed that water loss and drying shrinkage of foamed concrete appeared mostly in the early 7 d. The decreased values of drying shrinkage and autogenous shrinkage of 28 d on foamed concrete were up to 55. 3% and 48. 9%,when W /C was 0. 33. With W /C 0. 50,drying shrinkage of 28 d on foamed concrete decreased by 59. 1% to the most. And tiny expansion of foamed concrete happened when it was isolated from outside. The number of capillary pores in foamed concrete was decreased by adding S1 with W /C 0. 33 and 0. 50.When W /C was 0. 33,the number of small capillary pores reduced by adding S2,but the big ones with the pore size of about 30 nm increased. When W /C was 0. 50,S2 benefited to increasing the number of small capillary pores less than 4nm.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Grouting, Rheology, and Soil Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.