Thermoelectric properties of hydrothermal synthesized Bi-Te-Se alloys
Source abstract
Abstract
Bi-Te-Se alloys were synthesized by hydrothermal method at 473K for 24h.The synthesized powders were composed of two kinds of BiTe-Se ternary alloys with the same structure.The powders were hot pressed into pellets at 523K under 50MPa,which were composed of two phases too.Both the powders and pellets exhibited layered particles with the thickness of about 100nm. The doping concentration can be optimized by changing the content of Te.The materials have remarkably low thermal conductivity.The lowest lattice thermal conductivity was found to be 0.33W/m·K at 349K and the maximum ZT value 0.60 in Bi_2Te_(2.85)Se_(0.45).Improved thermoelectric properties could be expected by synthesizing anisotropic materials and doping with iodine based on this work.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Neural Networks and Applications · Advanced Thermoelectric Materials and Devices · Advanced Semiconductor Detectors and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.