Preparation of titanium carbide powders in high-frequency induction furnace
Source abstract
Abstract
Formation of ultrafine TiC powders by carbothermal reduction of titania and charcoal in high-frequency induction furnace was investigated by XRD, SEM/EDS, atomic Absorption spectrometer, XRF as well as laser particle sizer. The result indicates that ultrafine TiC powders with low impurities was prepared at temperature range 1490-1510℃ for a short time. The surface of TiC particles is homogeneous and loose agglomeration while the grain size (D50) is about 1-10μm. Lattice parameter calculation indicates that sub-stoichiometric TiCx(x1) should exist in TiC powders when n(TiO2)∶n(C)=1∶3. But stoichiometric TiC1.0 was prepared when n(TiO2)∶n(C)=1∶4.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Metallurgical and Alloy Processes · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.