Processes study on magnetization roasting method to strengthen whitening kaolin by magnetic separating removal iron method
Source abstract
Abstract
The experiment used magnetic roasting process,took bamboo charcoal powder that was dealt with base activator as magnetic roasting reducing agent.It studied that additive,sintering temperature,and holding time had some effects on mass susceptibility of iron mineral in kaolin.Determined finally the best solution of magnetic roasting process was that it was added 2.0% boric acid and 3.0% NaHCO3,its magnetic roasting temperature was about 450 ℃,its holding time was 30 min,and mass susceptibility of iron mineral in kaolin reached 5.58×10-4 m3/kg.To kaolin after treatment of magnetic roasting process,it was necessary to deal with it by wet milling.When the pH value in the slurry system was about 9and milling time was about 30 min.The production rate of magnetic separation was up to 84.4%.And this time the calcined whiteness of magnetic kaolin concentrate(Temperature was 1 200 ℃)was 87.4%.It increased by 22.6%than calcined whiteness 71.3% of untreated kaolin sample,it increased by 14.2%than calcined whiteness 76.5% of original kaolin sample.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Geoscience and Mining Technology
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.