Influence of Proximal-Cervical Undermined Enamel Areas on Marginal Quality and Enamel Integrity of Laboratory and CAD/CAM Ceramic Inlays and Partial Crowns
Source abstract
Abstract
(1) The aim of this in vitro study was to investigate the handling of proximal-cervical undermined enamel margins on the adhesive performance of differently fabricated and differently cemented ceramic inlays and partial crowns (2) Methods: 192 extracted third molars received MOD (n = 96) and partial crown (n = 96) preparations. A mesial 2 × 2 × 4 mm cervical groove was created in dentin to simulate a deeper (dentin) caries excavation. This dentin groove was either left (G/groove), filled with composite (F/filling), or completely removed (D/dentin). Distal proximal boxes did not receive a groove and served as controls within the same tooth. Labside (e.max Press) restorations additionally went through a temporary phase. Labside and chairside (e.max CAD) inlays and partial crowns were then adhesively luted with Syntac/Variolink Esthetic (SV) or Adhese Universal/Variolink Esthetic (AV). Initially, and again after thermomechanical loading (TML: 1 million cycles at 50 N, 25,000 thermocycles at 5 °C/55 °C), specimens were molded and the resulting 24 groups of epoxy replicas (n = 8) were gold-sputtered and examined for marginal gaps using scanning electron microscopy (200× magnification). Light microscopy (10× magnification) was used to measure proximal cervical crack propagation in adjacent enamel. (3) Results: Regardless of the adhesive system, D groups generally showed significantly lower marginal quality (79–88%; p < 0.05), with the universal adhesive performing better than the multi-step adhesive system (p < 0.05). Subgroups G and F were similar in marginal quality (94–98%; p > 0.05) and not worse than the controls (p > 0.05) regardless of the adhesive system, but showed less cracking in F than in G (p < 0.05). In general, fewer cracks were observed in chairside CAD/CAM restorations than in laboratory-fabricated restorations (p < 0.05). Partial crowns showed better marginal quality (96–98%) and less cracking than inlays (p < 0.05). (4) Conclusions: If the dentin level is lower than the enamel level in ceramic preparations after caries excavation in the proximal box, the resulting undermined enamel should not be removed. In terms of enamel integrity, partial crowns outperformed inlays.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Research and COVID-19
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Operative Dentistry, Endodontics, and Pediatric Dentistry, Medical Center for Dentistry, University Medical Center Giessen and Marburg, 35039 Marburg, Germany
Department of Paediatric Dentistry, Medical Center for Dentistry, University Medical Center Giessen and Marburg, Campus Giessen, Schlangenzahl 14, 35392 Giessen, Germany
References (31)
Show source-provided references
1. Long-term outcomes of all-ceramic inlays and onlays after a mean observation time of 11 years
2. A prospective 15-year evaluation of extensive dentin-enamel-bonded pressed ceramic coverages10.1016/j.dental.2010.05.008 ↗
3. Clinical performance of bonded ceramic inlays/onlays: A 5- to 18-year retrospective longitudinal study
4. Clinical performance of large, all-ceramic CAD/CAM-generated restorations after three years: A pilot study10.14219/jada.archive.2004.0248 ↗
5. Clinical results of Cerec inlays in a dental practice over a period of 18 years
6. A practice-based research network on the survival of ceramic inlay/onlay restorations10.1016/j.dental.2016.02.006 ↗
7. Effect of dentin moisture in posterior restorations performed with universal adhesive: A randomized clinical trial10.2341/20-215-C ↗
8. influence of adhesive type and placement technique on postoperative sensitivity in posterior composite restorations10.2341/16-010-C ↗
9. Influence of incorrect application of a water-based adhesive system on the marginal adaptation of Class V restorations
10. de Kuijper, M.C.F.M., Ong, Y., Gerritsen, T., Cune, M.S., and Gresnigt, M.M.M. (2021). Influence of the ceramic translucency on the relative degree of conversion of a direct composite and dual-curing resin cement through lithium disilicate onlays and endocrowns. J. Mech. Behav. Biomed. Mater., 122.10.1016/j.jmbbm.2021.104662 ↗
11. In vitro evaluation of marginal and internal adaptations of ceramic inlay restorations associated with immediate vs delayed dentin sealing techniques10.11607/ijp.6372 ↗
12. Guidelines for the preparation of CAD/CAM ceramic inlays and partial crowns
13. Interventions for treating cavitated or dentine carious lesions
14. Marginal gap behavior of composite and ceramic inlays in extended cavities
15. Chairside vs. labside ceramic inlays: Effect of temporary restoration and adhesive luting on enamel cracks and marginal integrity10.1016/j.dental.2011.05.007 ↗
16. Fatigue behavior of dental resin composites: Flexural fatigue in vitro versus 6 years in vivo
17. Efficacy of adhesive strategies for restorative dentistry: A systematic review and network meta-analysis of double-blind randomized controlled trials over 12 months of follow-up10.2186/jpr.JPR_D_21_00279 ↗
18. Carrilho, E., Cardoso, M., Marques Ferreira, M., Marto, C.M., Paula, A., and Coelho, A.S. (2019). 10-MDP Based Dental Adhesives: Adhesive Interface Characterization and Adhesive Stability-A Systematic Review. Materials, 12.10.3390/ma12050790 ↗
19. Do universal adhesives promote bonding to dentin? A systematic review and meta-analysis10.5395/rde.2018.43.e29 ↗
20. Effect of an additional bonding resin on the 5-year performance of a universal adhesive: A randomized clinical trial10.1007/s00784-022-04613-8 ↗
21. Universal adhesives benefit from an extra hydrophobic adhesive layer when light cured beforehand
22. The effect of curing mode of dual-cure resin cements on bonding performance of universal adhesives to enamel, dentin and various restorative materials10.4012/dmj.2020-077 ↗
23. Extra bonding layer compensates universal adhesive’s thin film thickness
24. Clinical and OCT assessment of application modes of a universal adhesive in a 12-month RCT10.1016/j.jdent.2022.104068 ↗
25. Clinical and OCT outcomes of a universal adhesive in a randomized clinical trial after 12 months10.1016/j.jdent.2019.103200 ↗
26. Partial glass-ceramic posterior restorations with margins beyond or above the cemento-enamel junction: An observational retrospective clinical study10.2186/jpr.JPR_D_23_00219 ↗
27. Up to 12 years clinical evaluation of 197 partial indirect restorations with deep margin elevation in the posterior region10.1016/j.jdent.2019.103227 ↗
28. Bresser, R.A., Carvalho, M.A., Naves, L.Z., Melma, H., Cune, M.S., and Gresnigt, M.M.M. (2024). Biomechanical behavior of molars restored with direct and indirect restorations in combination with deep margin elevation. J. Mech. Behav. Biomed. Mater., 152.10.1016/j.jmbbm.2024.106459 ↗
29. Periodontal health in teeth treated with deep-margin-elevation and CAD/CAM partial lithium disilicate restorations-a prospective controlled trial10.1007/s00784-024-06053-y ↗
30. Leucite-reinforced glass ceramic inlays and onlays after 12 years
31. A 10-year prospective evaluation of CAD/CAM-manufactured (Cerec) ceramic inlays cemented with a chemically cured or dual-cured resin composite