Bio-Environment-Induced Degradation and Failure of Internal Fixation Implants
Source abstract
Abstract
Internal fixations provide fast healing but their failure remains problematic to patients. Here, we report an experimental study in failure of three typical cases of metals: a bent intramedullary stainless steel nail, a broken exterior pure Ti plate, and a broken intramedullary stainless steel nail. Characterization of the bent nail indicates that those metals are vulnerable to corrosion with the evidence of increased surface roughness and embrittlement. Depredated surface of the Ti plate resulted debris particles in the surrounding tissue of 15.2 ± 6.5 μm in size. Nanoparticles were observed in transmission electron microscope. The electron diffraction pattern of the debris indicates a combination of nanocrystalline and amorphous phases. The failure mode of the broken nail made of stainless steel was found to be fatigue initiated from the surface. This study clearly shows the biological-attack induced surface degradation resulting in debris and fatigue. Future design and selection of implant materials should consider such factors for improvement.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Bone fractures and treatments · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Materials Science and Engineering, Texas A&M University, College Station, TX 77843, USA
Mechanical Engineering, Texas A&M University, College Station, TX 77843, USA
Department of Orthopedic Trauma, Shandong Provincial Hospital Affiliated to Shandong University, Jinan 250021, China
References (14)
Show source-provided references
1. Lieberman, J.R., and Friedlaender, G.E. (2007). Bone Regeneration and Repair: Biology and Clinical Applications, Humana Press Inc.
2. Ratner, B.D., Hoffman, A.S., Schoen, F.J., and Lemons, J.E. (2013). Biomaterials Science: An Introduction to Materials in Medicine, Academic Press.
3. Biomedical implants: Corrosion and its prevention—A review10.2174/1877610801002010040 ↗
4. Tissue-biomaterial interactions10.1007/BF01161439 ↗
5. Characteristics of metals used in implants10.1089/end.1997.11.383 ↗
6. Williams, D.F. (1981). Biocompatibility of Clinical Implant Materials, CRC Press.
7. The effect of particle phagocytosis and metallic wear particles on osteoclast formation and bone resorption in vitro10.1054/arth.2000.6622 ↗
8. Mediators of the inflammatory response to joint replacement devices10.1038/nrrheum.2011.128 ↗
9. Wear debris characterization and corresponding biological response: Artificial hip and knee joints10.3390/ma7020980 ↗
10. Polyethylene wear particles in synovial fluid after total knee arthroplasty10.1097/01.blo.0000063122.39522.c2 ↗
11. Metal wear particle characterization from metal on metal total hip replacements: Transmission electron microscopy study of periprosthetic tissues and isolated particles10.1002/(SICI)1097-4636(199810)42:1<103::AID-JBM13>3.0.CO;2-M ↗
12. Applications of plasma coatings in artificial joints: An overview10.1016/j.vacuum.2003.12.160 ↗
13. Tribological performance of some alternative bearing materials for artificial joints10.1016/S0043-1648(03)00276-X ↗
14. Potential application of a Ti–C:H coating in implants10.1111/j.1551-2916.2011.05000.x ↗