Abstract

Silicon carbide fibers have superior flexural properties and chemical stability compared to glass fibers. We investigated the flexural strength and modulus of an experimental, short silicon carbide fiber-reinforced resin. Short silicon carbide fibers with lengths of ~0.5, 1, 2, and 3 mm were prepared and silanized. Urethane dimethacrylate and triethylene glycol dimethacrylate were mixed at a 70:30 wt% ratio and used as the matrix resins. Each length of short silicon carbide fibers and the matrix resin were combined using a mixing machine and then used for specimen preparation. The three-point bending test conditions were in accordance with ISO 4049:2009. The fracture surfaces of the specimens after the three-point bending test were observed using secondary electron images. The data were statistically analyzed with a one-way analysis of variance and Tukey’s HSD test (α = 0.05). The flexural strength and modulus of the specimens containing 2 mm or 3 mm silicon carbide fibers were significantly higher than the other specimens. The river pattern was observed more clearly in specimens containing shorter silicon carbide fibers, although this pattern was observed in all specimens.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Mechanical Behavior of Composites · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Division of Preventive Dentistry, Faculty of Dentistry, Graduate School of Medical and Dental Sciences, Niigata University, 2-5274 Gakkocho-dori, Chuo-ku, Niigata 951-8514, Japan

Division of Bio-Prosthodontics, Faculty of Dentistry, Graduate School of Medical and Dental Sciences, Niigata University, 2-5274 Gakkocho-dori, Chuo-ku, Niigata 951-8514, Japan

Division of Biomimetics, Faculty of Dentistry, Graduate School of Medical and Dental Sciences, Niigata University, 2-5274 Gakkocho-dori, Chuo-ku, Niigata 951-8514, Japan

Funding

Japan Society for the Promotion of Science

References (42)

Show source-provided references
1. Two-year clinical comparison of a flowable-type nano-hybrid composite and a paste-type composite in posterior restoration10.1111/jicd.12227 ↗
2. Correction to: Eight-year clinical evaluation of two types of resin composite in non-carious cervical lesions10.1007/s00784-022-04621-8 ↗
3. Longevity of Direct Resin Composite Restorations in Maxillary Anterior Crown Fractures: A 4-year Clinical Evaluation10.2341/20-162-C ↗
4. Three-year clinical evaluation of a flowable and a hybrid resin composite in non-carious cervical lesions10.1016/j.jdent.2009.10.003 ↗
5. A report on the clinical use of bonding systems for coronal restorations produced from CAD/CAM resin blocks10.4012/dmj.2019-277 ↗
6. Four-year clinical evaluation of CAD/CAM indirect resin composite premolar crowns using 3D digital data: Discovering the causes of debonding10.2186/jpr.JPR_D_20_00287 ↗
7. The effect of fiber orientation on the thermal expansion coefficients of fiber-reinforced composites10.1016/S0109-5641(02)00092-1 ↗
8. Finite element analysis of the possible mechanism of cervical lesion formation by occlusal force10.1046/j.1365-2842.2003.00959.x ↗
9. Reinforcement of conventional glass-ionomer restorative material with short glass fibers10.1016/j.jmbbm.2008.04.002 ↗
10. Reinforcement of denture base resin with short-rod glass fiber10.4012/dmj.26.733 ↗
11. Comparison of fiber-reinforced composite and nanohybrid resin impregnated with glass fibers as postendodontic restoration in molars-A clinical study10.4103/jcd.jcd_147_21 ↗
12. Clinical Evaluation of Fiber-Reinforced Composite Restorations in Posterior Teeth-Results of 2.5 Year Follow-up10.2174/1874210601812010476 ↗
13. Hardness and fracture toughness of resin-composite materials with and without fibers10.1016/j.dental.2019.05.017 ↗
14. Effect of 180-week water storage on the flexural properties of E-glass and silica fiber acrylic resin composite
15. Study of Strength Degradation Mechanism of Woven GFRP in Water Environment10.1299/jmmp.4.1574 ↗
16. Tensile properties of heat-treated Nicalon and Hi-Nicalon fibres10.1016/S1359-835X(01)00125-7 ↗
17. Mechanical and structural characterization of the Nicalon silicon carbide fibre10.1007/PL00020090 ↗
18. Comparison of mechanical properties of glass fiber/vinyl ester and carbon fiber/vinyl ester composites10.1016/j.compositesb.2005.01.004 ↗
19. Effects of silane coupling agent amount on mechanical properties and hydrolytic durability of composite resin after hot water storage10.4012/dmj.23.31 ↗
20. Effect of silane coupling agent and concentration on fracture toughness and water sorption behaviour of fibre-reinforced dental composites10.1016/j.dental.2023.03.002 ↗
21. Effects of Silanization Conditions on Flexural Properties of Sic Fiber-Reinforced Resin10.4172/2161-1122.1000524 ↗
22. Discontinuous fiber-reinforced composites above critical length10.1177/154405910508400414 ↗
23. Mechanical and structural characterization of discontinuous fiber-reinforced dental resin composite10.1016/j.jdent.2016.07.009 ↗
24. Radiopacity of experimental composite resins containing radiopaque materials10.4012/dmj.24.315 ↗
25. The effect of fiber orientation on the toughening of short fiber-reinforced polymers10.1002/app.12913 ↗
26. Physical properties and depth of cure of a new short fiber reinforced composite10.1016/j.dental.2013.04.016 ↗
27. Short fiber reinforced composite: The effect of fiber length and volume fraction10.5005/jcdp-7-5-10 ↗
28. Effects of Manufacturing-Induced Voids on Local Failure in Polymer-Based Composites10.1115/1.2841529 ↗
29. The effect of voids on the quasi-static tensile properties of carbon fiber/polymer-laminated composites10.1177/0021998317737827 ↗
30. A comparison process between hand lay-up, vacuum infusion and vacuum bagging method toward e-glass EW 185/lycal composites10.1088/1742-6596/1130/1/012018 ↗
31. Influence of working environment and built orientation on the tensile properties of selective laser melted AlSi10Mg alloy10.1016/j.msea.2019.01.103 ↗
32. Brittle–tough transition of rapid crack propagation in polyethylene10.1016/S0032-3861(97)10336-6 ↗
33. Physicochemical properties of discontinuous S2-glass fiber reinforced resin composite10.4012/dmj.2017-078 ↗
34. Mechanical properties of dental resin/composite containing urchin-like hydroxyapatite10.1016/j.dental.2014.10.003 ↗
35. Investigations on mechanical behaviour of dental composites10.1007/s00784-009-0258-4 ↗
36. Mechanical properties of fiber reinforced restorative composite with two distinguished fiber length distribution10.1016/j.jmbbm.2016.01.036 ↗
37. Continuous-fiber preform reinforcement of dental resin composite restorations10.1016/S0109-5641(02)00100-8 ↗
38. Mechanical properties of palmyra/glass fiber hybrid composites10.1016/j.compositesa.2007.06.006 ↗
39. Flexural properties of experimental nanofiber reinforced composite are affected by resin composition and nanofiber/resin ratio10.1016/j.dental.2015.06.018 ↗
40. Structure-property relationships in dimethacrylate networks based on Bis-GMA, UDMA and TEGDMA10.1016/j.dental.2009.01.106 ↗
41. Mechanical properties, accuracy, and cytotoxicity of UV-polymerized 3D printing resins composed of Bis-EMA, UDMA, and TEGDMA10.1016/j.prosdent.2019.05.002 ↗
42. Post-cure heat treatments for composites: Properties and fractography10.1016/0109-5641(92)90102-I ↗