The Impact of Additive and Subtractive Manufacturing on the Adhesion and Durability of Titanium–Zirconia Restorative Materials
Source abstract
Abstract
This study aimed to investigate the bonding strength and durability of titanium alloys bonded to zirconia-based materials produced using subtractive and additive digital methods. Two titanium alloy groups (N = 20) and two zirconia ceramic groups (N = 60) were fabricated using CAD/CAM milling from prefabricated discs (Ti-ML and Zr-ML), and 3D printing via SLM (Ti-3D) and DLP/LCM systems (Zr-3D). The specimens were bonded with dental cement to form four test groups: Zr-ML/Ti-ML, Zr-ML/Ti-3D, Zr-3D/Ti-ML, and Zr-3D/Ti-3D. Half of the specimens in each group underwent thermocycling to assess the effect of aging on bond strength. The density, microhardness, and surface morphology were evaluated, along with the shear bond strength and failure modes of the resin composites. Statistical differences were analyzed using one-way ANOVA and Tukey’s HSD test across all groups. The 3D-printed specimens of both materials exhibited higher microhardness and lower surface roughness than the milled specimens. The shear bond strength (SBS) was the highest in the Ti-ML/Zr-ML combination group before and after thermocycling, which had more cohesive failures, whereas the lowest bond strength was observed in the Ti-3D/Zr-ML group. The adhesion between titanium and zirconia-based materials was the strongest when both were fabricated using subtractive methods, followed by additive and mixed-method combinations.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Additive Manufacturing and 3D Printing Technologies · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Dental Health Department, College of Applied Medical Sciences, King Saud University, P.O. Box 10219, Riyadh 11433, Saudi Arabia
Funding
King Saud University, Riyadh, Saudi Arabia
References (34)
Show source-provided references
1. Zirconia versus titanium in dentistry: A review10.4012/dmj.2019-172 ↗
2. Bond durability and surface states of titanium, Ti-6Al-4V alloy, and zirconia for implant materials10.2186/jpr.JPR_D_20_00297 ↗
3. Comparison of the shear bond strength of composite resins with zirconia and titanium using different resin cements10.2186/jpr.JPR_D_20_00299 ↗
4. Microstructural homogeneity and mechanical behavior of a selective laser melted Ti-35Nb alloy produced from an elemental powder mixture10.1016/j.jmst.2020.05.052 ↗
5. In vitro investigation of shear bond strength of titanium alloy bonded to monolithic zirconia prepared via different surface roughening methods using different cements10.33808/clinexphealthsci.1216743 ↗
6. Titanium versus zirconia complete arch implant-supported fixed prostheses: A comparison of plaque accumulation10.1016/j.prosdent.2021.10.012 ↗
7. Shear bond strength of zirconia-based ceramics veneered with 2 different techniques10.1016/j.prosdent.2016.11.016 ↗
8. Shen, D., Wang, H., Shi, Y., Su, Z., Hannig, M., and Fu, B. (2023). The effect of surface treatments on zirconia bond strength and durability. J. Funct. Biomater., 14.10.3390/jfb14020089 ↗
9. Adhesion of Streptococcus mutans on highly translucent zirconia: Influence of surface properties and polyelectrolyte multilayer coatings10.1016/j.prosdent.2025.01.038 ↗
10. Effect of milled and lithography-based additively manufactured zirconia (3Y-TZP) on the biological properties of human osteoblasts10.1016/j.prosdent.2022.01.025 ↗
11. Three-dimensional printing technologies for dental prosthesis: A review10.1108/RPJ-07-2021-0164 ↗
12. Accuracy, fit, and marginal quality of advanced additively manufactured and milled zirconia 3-unit fixed dental prostheses10.1016/j.prosdent.2024.09.016 ↗
13. Shear bond strength of adhesive cement to zirconia: Effect of added proportion of yttria for stabilization10.1016/j.prosdent.2024.02.010 ↗
14. Alageel, O., Alfrisany, N., Aldosari, A., Qashish, S., Alsarani, M.M., and AlFaify, A.Y. (2024). Impact of density variations and growth direction in 3D-printed titanium alloys on surface topography and bonding performance with dental resins. Crystals, 14.10.3390/cryst14080712 ↗
15. Removable partial denture alloys processed by laser-sintering technique10.1002/jbm.b.33929 ↗
16. Sokolowski, G., Szczesio-Wlodarczyk, A., Szynkowska-Jóźwik, M.I., Stopa, W., Sokolowski, J., Kopacz, K., and Bociong, K. (2023). The shear bond strength of resin-based luting cement to zirconia ceramics after different surface treatments. Materials, 16.10.3390/ma16155433 ↗
17. Retention of zirconia crowns to Ti-base abutments: Effect of luting protocol, abutment treatment and autoclave sterilization10.2186/jpr.JPOR_2019_537 ↗
18. Accuracy of zirconia crowns manufactured by stereolithography with an occlusal full-supporting structure: An in vitro study10.1016/j.prosdent.2022.01.015 ↗
19. 3D printing of zirconia–what is the future?10.1007/s40496-019-00243-4 ↗
20. Alageel, O., Alhijji, S., Alsadon, O., Alsarani, M., Gomawi, A.A., and Alhotan, A. (2023). Trueness, flexural strength, and surface properties of various three-dimensional (3D) printed interim restorative materials after accelerated aging. Polymers, 15.10.3390/polym15143040 ↗
21. Design, defect analysis, compressive strength and surface texture characterization of laser powder bed fusion processed Ti6Al4V lattice structures10.1016/j.jmrt.2025.01.232 ↗
22. Critical evaluation of the pulsed selective laser melting process when fabricating Ti64 parts using a range of particle size distributions
23. Moon, J.M., Jeong, C.S., Lee, H.J., Bae, J.M., Choi, E.J., Kim, S.T., Park, Y.B., and Oh, S.H.A. (2022). A comparative study of additive and subtractive manufacturing techniques for a zirconia dental product: An analysis of the manufacturing accuracy and the bond strength of porcelain to zirconia. Materials, 15.10.3390/ma15155398 ↗
24. Schwickerath adhesion tests of porcelain veneer and stereolithographic additive-manufactured zirconia10.1016/j.ceramint.2020.03.228 ↗
25. (2013). Standard Test Method for Apparent Density of Free-Flowing Metal Powders Using the Hall Flowmeter Funnel. Standard No. ASTM B212-13.
26. The influence of recycling on the properties of interface between ceramic and dental alloys10.1155/2020/3529781 ↗
27. Effect of adhesive system, resin cement, heat-pressing technique, and thermomechanical aging on the adhesion between titanium base and a high-performance polymer10.1016/j.prosdent.2022.03.026 ↗
28. Effects on microhardness, tensile strength, deflection, and drop weight impact resistance with the addition of hybrid filler materials for enhancing GFRP composites10.1038/s41598-024-76094-6 ↗
29. Park, Y., Kim, J., Kang, Y.-J., Shim, E.-Y., and Kim, J.-H. (2024). Comparison of fracture strength of milled and 3D-printed crown materials according to occlusal thickness. Materials, 17.10.3390/ma17184645 ↗
30. Cherneva, S., Petrunov, V., Petkov, V., Bogdanov, V., and Simeonova, S. (2023). Structure and mechanical properties of milled and 3D-printed Ti-6Al-4V alloys for subtractive and additive CAD/CAM manufacturing in dentistry. Appl. Sci., 13.10.20944/preprints202310.0629.v1 ↗
31. Improving the surface characteristics of additively manufactured parts: A review10.1016/j.matpr.2021.04.223 ↗
32. Shear bond strength and failure modes of composite to dentin under different light-curing conditions
33. In vitro evaluation of shear bond strength of three primer/resin cement systems to monolithic zirconia10.11607/ijp.6258 ↗
34. In vitro shear bond strength of two self-adhesive resin cements to zirconia10.1016/j.prosdent.2014.08.006 ↗