Mechanical and Tribological Characterization of a Dental Ceromer

Mariana Santos, Ana Sofia Coelho, Anabela Baptista Paula, Carlos Miguel Marto, Inês Amaro, José Saraiva, Manuel Marques Ferreira, Pedro Antunes, Eunice Carrilho

Abstract

Background: Indirect restorations using composites with ceramic fillings can be an alternative to ceramic veneering and direct composite restorations for the treatment of posterior teeth. The aim of this study was the evaluation of the mechanical and tribological properties of a ceromer. Materials and Methods: Sixty specimens were produced and divided into two groups: one control group not submitted to thermocycling (n = 20) and one test group submitted to 5000 cycles of thermocycling (n = 40). The studied parameters were microhardness, surface roughness and the coefficient of friction (scratch test). Results: The ceromer exhibits a reduction of polymerization shrinkage, higher wear, and fracture resistance than the composite resins. The studied ceromer presented good mechanical properties, even after being submitted to thermocycling. Roughness was the property most affected, increasing 25.8%, microhardness decreased by 10.5% and the coefficient of friction increased by 4.2%. Conclusions: In certain situations, ceromers can be an alternative to composite resins and ceramics, providing an aesthetic, conservative and longevity option.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Environmental and biological studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Integrated Clinical Practice, Faculty of Medicine, University of Coimbra, 3000-075 Coimbra, Portugal

Institute for Clinical and Biomedical Research (iCBR), Area of Environment, Genetics and Oncobiology (CIMAGO), Faculty of Medicine, University of Coimbra, 3000-548 Coimbra, Portugal

CNC.IBILI Consortium, Faculty of Medicine, University of Coimbra, 3000-548 Coimbra, Portugal

Centre for Innovative Biomedicine and Biotechnology (CIBB), University of Coimbra, 3000-548 Coimbra, Portugal

Institute of Experimental Pathology, Faculty of Medicine, University of Coimbra, 3000-548 Coimbra, Portugal

Institute of Endodontics, Faculty of Medicine, University of Coimbra, 3000-075 Coimbra, Portugal

Department of Mechanical Engineering, Centre for Mechanical Engineering, Materials and Processes (CEMMPRE), University of Coimbra, 3030-788 Coimbra, Portugal

Itecons—Institute of Research and Technological Development in Construction, Energy, Environment and Sustainability, Rua Pedro Hispano, 3030-289 Coimbra, Portugal

References (31)

Show source-provided references
1. Developing an intracoronal restoration with indirect composite resin. Part 2
2. Effect of two abrasive systems on resin bonding to laboratory-processed indirect resin composite restorations10.1111/j.1708-8240.1999.tb00398.x ↗
3. Zafar, M.S., Khurshid, Z., Najeeb, S., Zohaib, S., and Rehman, I.U. (2017). Therapeutic Applications of Nanotechnology in Dentistry. Nanostructures for Oral Medicine, Elsevier.10.1016/B978-0-323-47720-8.00027-4 ↗
4. Advances in Nanotechnology for Restorative Dentistry10.3390/ma8020717 ↗
5. Antunes, P.A.A.V. (2012). Physical-Mechanical Characterization of Direct Restorative Dental Materials. [Ph.D. Thesis, University of Coimbra].
6. Thermocycling effect on mechanical and tribological characterization of two indirect dental restorative materials10.1007/s40430-016-0579-6 ↗
7. Water sorption and solubility of dental composites and identification of monomers released in an aqueous environment10.1046/j.1365-2842.2001.00802.x ↗
8. The relationship between physical parameters and wear of dental composites10.1016/j.wear.2006.12.010 ↗
9. Evaluation of fracture resistance of endodontically treated maxillary premolars, restored with ceromer or heat-pressed ceramic inlays and fixed with dual-resin cements10.1046/j.1365-2842.2003.01239.x ↗
10. Short-term clinical evaluation of inlay and onlay restorations made with a ceromer
11. Clinical study comparing at 5 years a ceramic and a ceromer used for making esthetic inlays
12. In vivo and in vitro evaluation of marginal fit of class II ceromer inlays10.1111/j.1365-2842.2005.01562.x ↗
13. A prospective clinical study of ceromer inlays: Results up to 53 months
14. Influence of shade and storage time on the flexural strength, flexural modulus, and hardness of composites used for indirect restorations10.1067/mpr.2001.114513 ↗
15. Marginal accuracy and fracture strength of ceromer/fiber-reinforced composite crowns: Effect of variations in preparation design10.1067/mpr.2002.128378 ↗
16. Effect of finish line variants on marginal accuracy and fracture strength of ceramic optimized polymer/fiber-reinforced composite crowns10.1016/j.prosdent.2004.03.004 ↗
17. Marginal adaptation of inlay-retained adhesive fixed partial dentures after mechanical and thermal stress: An in vitro study10.1067/mpr.2001.115072 ↗
18. Effect of tooth brushing and thermal cycling on a surface change of ceromers finished with different methods10.1046/j.1365-2842.2002.00877.x ↗
19. Inlay fixed partial denture as a conservative approach for restoring posterior missing teeth: A clinical report10.1016/S0022-3913(03)00117-3 ↗
20. Effect of mouth-motion fatigue and thermal cycling on the marginal accuracy of partial coverage restorations made of various dental materials10.1016/j.dental.2008.02.005 ↗
21. Comparison of the fracture strengths of metal-ceramic crowns and three ceromer crowns10.1067/mpr.2002.127712 ↗
22. Standard, A.S.T.M. (2000). E384 Standard Test Method for Microindentation Hardness of Materials. West Conshohocken PA ASTM Int., 1–40.
23. Dependence of Vickers microhardness on applied load in indium10.1023/A:1018533131255 ↗
24. EN ISO-4287 (1997). Geometrical Product Specifications (GPS)—Surface Texture: Profile method—Terms, Definitions and Surface Texture Parameters, International Organization for Standardization (ISO).
25. G171 Standard test method for scratch hardness of materials using a diamond stylus
26. Deformation behavior of human enamel and dentin–enamel junction under compression10.1016/j.msec.2013.10.009 ↗
27. The effect of different insertion techniques on the depth of cure and vickers surface micro-hardness of two bulk-fill resin composite materials
28. Effects of coating with different ceromers on the impact strength, transverse strength and elastic modulus of polymethyl methacrylate10.4012/dmj.2014-203 ↗
29. Neto, J. (2012). Metrologia e Controle Dimensional, Elsevier. [1st ed.].
30. Peixoto, D.F.C. (2008). Estudo do Contacto Roda/Carril: Análise de Tensões e Fadiga, Universidade do Porto.
31. The effect of surface roughness on ceramics used in dentistry: A review of literature10.4103/1305-7456.143646 ↗