Effect of Storage Temperature on Selected Strength Parameters of Dual-Cured Composite Cements
Source abstract
Abstract
Direct restorations are currently the most popular restorations used in dental prosthodontics. Due to the increased requirements for materials used in the fabrication of fixed restorations, there is a need for evaluation of strength parameters of these materials, including dental cements. The present study investigated the change in selected strength parameters of four dual-cured composite cements as a function of storage temperature. The following were investigated: three-point flexural strength (FS), flexural modulus in bending (FM), diametral tensile strength (DTS) and Vickers hardness (HV). Four dual-cured composite cements were tested, i.e., Multilink Automix (Ivoclar Vivadent), seT PP (SDI), MaxCem (Kerr), and Bifix Hybrid Abutment (VOCO). Each of the tested cements was stored for 7 days at one of the selected temperatures: 8 °C, 15 °C, 25 °C, or 35 °C, before the samples were made. Strength properties (DTS, FS) are not strongly dependent on the storage temperature in the range of 8–35 °C. Some statistical differences were observed between the hardness of MaxCem and Multilink Automix storage in various temperatures. FS and FM were lowest for Bifix Hybrid Abutment, MaxCem and Multilink Automix storage at 25 °C, and highest for Bifix Hybrid Abutment, MaxCem, and seT PP stored in 35 °C. The cement with the highest filler content (70% by weight) showed the highest FS and HV.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Bone Tissue Engineering Materials · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Prosthodontics, Medical University of Lodz, 92-213 Łódź, Poland
University Laboratory of Materials Research, Medical University of Lodz, 92-213 Łódź, Poland
Department of General Dentistry, Medical University of Lodz, 92-213 Łódź, Poland
References (43)
Show source-provided references
1. The temperature of cement specimens and its influence on measured strength10.1016/S0109-5641(85)80029-4 ↗
2. Effect of pre-heated dual-cured resin cements on the bond strength of indirect restorations to dentin10.1590/S1806-83242012000200014 ↗
3. Heat transfer properties and thermal cure glass-ionomer dental cements10.1007/s10856-015-5578-0 ↗
4. Curing dental resin and composites by photopolymerization10.1111/j.1708-8240.2000.tb00239.x ↗
5. Degree of conversion and residual stress of preheated and room-temperature composites10.4103/0970-9290.35827 ↗
6. Pre-heating of high-viscosity bulk-fill resin composites: Effects on shrinkage force and monomer conversion10.1016/j.jdent.2015.07.014 ↗
7. Effect of heat on the flow of commercial composites
8. Effect of pre-heating composite resin on gap formation at three different temperatures10.4103/0972-0707.82618 ↗
9. Effect of preheating and light-curing unit on physicochemical properties of a bulk-fill composite10.2147/CCIDE.S130803 ↗
10. Post-gel shrinkage strain and degree oh conversion of preheated resin composite cured using different regimens10.2341/09-072-L ↗
11. Effect of preheating on the viscoelastic properties of dental composite under different deformation conditions10.4012/dmj.2015-042 ↗
12. Effect of storage temperature on the shelf life of self-adhesive resin cements
13. Comparative analysis of selected mechanical properties of preheated composite material and self-adhesive composite cement—Pilot study10.5114/ps/127074 ↗
14. Skąpska, A., Komorek, Z., Cierech, M., and Mierzwińska-Nastalska, E. (2022). Comparison of mechanical properties of self-adhesive composite cement and heated composite material. Polymers, 14.10.3390/polym14132686 ↗
15. Atomic vibrational origins of mechanical toughness in bioactive cement during settin10.1038/ncomms9631 ↗
16. Chemical actinometry (IUPAC Technical Report)10.1351/pac200476122105 ↗
17. Gender differences in thermal comfort and use of thermostats in everyday thermal environments10.1016/j.buildenv.2006.01.009 ↗
18. Absolute Temperature Thresholds for Detection of Skin Wetness and Dampness on the Hand and their Variation with Sex and Age10.1177/03010066211043467 ↗
19. A sex/age anomaly in thermal comfort observed in an office worker field study: A menopausal effect?
20. Pre-heated dual-cured resin cements: Analysis of the degree of conversion and ultimate tensile strength10.1590/S1806-83242011000200013 ↗
21. Machanical properties of new self-adhesive resin-based cement10.1016/j.jpor.2009.09.004 ↗
22. Physical Properties and Comperative Strength of a Bioactive Luting Cement
23. Clinically relevant issues related to preheating composites10.1111/j.1708-8240.2006.00046.x ↗
24. Effect of preheating and precooling on the flexural strength and modulus of elasticity of nanohybrid and silorane-based composite
25. Comperative evaluation of mechanical properties of resin, self-adhesive and adhesive cements
26. Effect of activation modes in the compressive strength, diametral tensile strength and microhardness od dual-cured self-adhesive resin cements10.4012/dmj.2015-056 ↗
27. A study on the characteristics of resin composites for provisional restorations10.4012/dmj.2021-006 ↗
28. A study of the physical and chemical properties of four resin composite luting cements
29. Pre-warming of dental composites10.1016/j.dental.2010.11.009 ↗
30. Effect of repeated preheating cycles on flexural strength of resin composites10.2341/11-476-L ↗
31. Surface microhardness of a self-adhesive composite in comparison with conventional composite resins10.17219/dmp/118123 ↗
32. Tzanakakis, E.G., Dimitriadi, M., Tzoutzas, I., Koidis, S., Zinelis, S., and Eliades, G. (2021). Effect of water storage on hardness and interfacial strength of resin composite luting agents bonded to surface—Treated monolithic zirconia. Dent. J., 7.10.3390/dj9070078 ↗
33. Properties and risk of the use of Bisphenol A-Glycidyl Methacrylate and Urethane Dimethacrylate—Basic monomers of dental restorative materials
34. Qualitative analysis of dental resin composites by gas and liquid chromatography/mass spectrometry10.1007/BF00323665 ↗
35. Identification of organic eluates from four polymerbased dental filling materials10.1034/j.1600-0722.2003.00033.x ↗
36. Biocompatibility of resin–modified filling materials10.1177/10454411000110030401 ↗
37. Substances released from dental resin composites and glass ionomer cements10.1046/j.0909-8836.1998.eos10602ii04.x ↗
38. Szczesio-Wlodarczyk, A., Polikowski, A., Krasowski, M., Fronczek, M., Sokolowski, J., and Bociong, K. (2022). The Influence of Low-Molecular-Weight Monomers (TEGDMA, HDDMA, HEMA) on the Properties of Selected Matrices and Composites Based on Bis-GMA and UDMA. Materials, 15.10.3390/ma15072649 ↗
39. Cements and Adhesives for All-Ceramic Restorations10.1016/j.cden.2011.01.011 ↗
40. Effects of temperature change on the working and and setting characteristics of water-based dental cements10.1016/S0109-5641(87)80087-8 ↗
41. Effects of temperature and aging on working/setting time of dual-resin cements10.2341/13-361-L ↗
42. Resin-modified glass-ionomer setting reaction competition10.1177/0022034509355919 ↗
43. Thermal analysis on the cure speed of dual cured resin cements under porcelain inlays10.1046/j.1365-2842.2001.00639.x ↗