journal article·2025-04-12Open access

An Assessment of the Micro-Tensile Bond Strength of Composites for Indirect Restoration to Enamel and Dentin

Viktoria Petrova, Janet Kirilova, Sevda Yantcheva

Abstract

This study aimed to evaluate the micro-tensile bond strength (µTBS) of two types of composites for indirect restoration, luted to enamel and dentin with self-adhesive cement. Moreover, it aimed to evaluate the impact of thermocycling on bond strength. Sixteen flat enamel and dentin surfaces of human molars were cemented to equal flat specimens of the laboratory composite Signum ceramis and the CAD/CAM block Cerasmart. Half of the specimens of the group underwent thermocycling. After that, the samples were cut into 80 beams for µTBS analysis. The data were analyzed using Levene’s test and the independent sample t-test. The micro-tensile bond strength tests revealed that thermocycling significantly reduced the adhesive bond. Dentin bonds better to conventional laboratory composites. Enamel bonds are better than composite blocks for milling.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Erosion and Treatment

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Conservative Dentistry, Faculty of Dental Medicine, Medical University, 1000 Sofia, Bulgaria

Funding

Bulgarian Ministry of Education and Science

References (51)

Show source-provided references
1. El-Askary, F., Hassanein, A., Aboalazm, E., Al-Haj Husain, N., and Özcan, M. (2022). A Comparison of Microtensile Bond Strength, Film Thickness, and Microhardness of Photo-Polymerized Luting Composites. Materials, 15.10.3390/ma15093050 ↗
2. Haruyama, A., Muramatsu, T., and Kameyama, A. (2024). The Effect of Silane Treatment of a Resin-Based Composite on Its Microtensile Bond Strength to a Ceramic Restorative Material. Appl. Sci., 14.10.3390/app14209178 ↗
3. Microleakage studies comparing a one-visit indirect composite inlay system and a direct composite restorative technique10.1111/j.1365-2842.1992.tb01101.x ↗
4. Marginal adaptation and microtensile bond strength of composite indirect restorations bonded to dentin treated with adhesive and low-viscosity composite10.1016/j.dental.2006.01.028 ↗
5. Spatio-temporal analysis of shrinkage vectors during photo-polymerization of composite10.1016/j.dental.2013.09.011 ↗
6. Sorption, solubility, shrinkage and mechanical properties of low-shrinkage commercial resin composites10.1016/j.dental.2013.01.006 ↗
7. Mechanical properties of composite resin blocks for CAD/CAM10.4012/dmj.2014-208 ↗
8. Resin composite blocks via high-pressure high-temperature polymerization10.1016/j.dental.2011.12.003 ↗
9. Indirect resin composites10.4103/0972-0707.73377 ↗
10. A comparison of the wear resistance and hardness of indirect composite resins10.1067/mpr.2001.114267 ↗
11. Dikici, B., Türkeş Başaran, E., and Can, E. (2025). Does the Type of Resin Luting Material Affect the Bonding of CAD/CAM Materials to Dentin?. Dent. J., 13.10.3390/dj13010041 ↗
12. A review of dental CAD/CAM: Current status and future perspectives from 20 years of experience10.4012/dmj.28.44 ↗
13. A systematic review of CAD/CAM fit restoration evaluations10.1111/joor.12205 ↗
14. Materials for chairside CAD/CAM-produced restorations10.14219/jada.archive.2006.0397 ↗
15. Paradigm™ (2000). MZ100 Block: Technical Product Profile, 3M ESPE.
16. Mechanical properties of resin-ceramic CAD/CAM restorative materials10.1016/j.prosdent.2015.04.016 ↗
17. Antoniou, I., Mourouzis, P., Dionysopoulos, D., Pandoleon, P., and Tolidis, K. (2024). Influence of Immediate Dentin Sealing on Bond Strength of Resin-Based CAD/CAM Restoratives to Dentin: A Systematic Review of In Vitro Studies. Biomimetics, 9.10.3390/biomimetics9050267 ↗
18. Microtensile bond strength of CAD/CAM materials to dentin under different adhesive strategies
19. Influence of different surface sreatments to Self-adhesive resin cement to CAD-CAM materials bonding
20. Papadopoulos, K., Pahinis, K., Saltidou, K., Dionysopoulos, D., and Tsitrou, E. (2020). Evaluation of the Surface Characteristics of Dental CAD/CAM Materials after Different Surface Treatments. Materials, 13.10.3390/ma13040981 ↗
21. Dental Cements for Luting and Bonding Restorations: Self-Adhesive Resin Cements10.1016/j.cden.2017.06.006 ↗
22. Wu, C.-Y., Nakamura, K., Miyashita-Kobayashi, A., Haruyama, A., Yokoi, Y., Kuroiwa, A., Yoshinari, N., and Kameyama, A. (2024). The Effect of Additional Silane Pre-Treatment on the Microtensile Bond Strength of Resin-Based Composite Post-and-Core Build-Up Material. Appl. Sci., 14.10.3390/app14156637 ↗
23. Awad, M.M., Alhalabi, F., Alshehri, A., Salem, M.A., Robaian, A., Alghannam, S., Alayad, A.S., Almutairi, B., and Alrahlah, A. (2023). Silane-Containing Universal Adhesives Influence Resin-Ceramic Microtensile Bond Strength. Coatings, 13.10.3390/coatings13020477 ↗
24. Adhesion of resin composite to enamel and dentin: A methodological assessment10.1080/01694243.2017.1354494 ↗
25. Chin, A., Ikeda, M., Takagaki, T., Nikaido, T., Sadr, A., Shimada, Y., and Tagami, J. (2021). Effects of Immediate and Delayed Cementations for CAD/CAM Resin Block after Alumina Air Abrasion on Adhesion to Newly Developed Resin Cement. Materials, 14.10.3390/ma14227058 ↗
26. Evaluation of Microtensile Bond Strength of Luting Cements to Zirconia Ceramics
27. Nakazawa, M., Maeno, M., Komoto, M., and Nara, Y. (2022). Appropriate Immediate Dentin Sealing to Improve the Bonding of CAD/CAM Ceramic Crown Restorations. Polymers, 14.10.3390/polym14214541 ↗
28. The microtensile bond strength test: Its historical background and application to bond testing10.1016/j.jdsr.2019.10.001 ↗
29. Relationship between bond-strength tests and clinical outcomes10.1016/j.dental.2009.11.148 ↗
30. The phenomena of rupture and flow in solids
31. Academy of Dental Materials guidance on in vitro testing of dental composite bonding effectiveness to dentin/enamel using micro-tensile bond strength (μTBS) approach10.1016/j.dental.2016.11.015 ↗
32. Gailani, H.F.A., Benavides-Reyes, C., Bolaños-Carmona, M.V., Rosel-Gallardo, E., González-Villafranca, P., and González-López, S. (2021). Effect of Two Immediate Dentin Sealing Approaches on Bond Strength of Lava™ CAD/CAM Indirect Restoration. Materials, 14.10.3390/ma14071629 ↗
33. Evaluation of micro-tensile bond strength of indirect resin composite inlay to dentin
34. Influence of specimen designs on the microtensile bond strength to dentin
35. Meta-analytical review of parameters involved in dentin bonding10.1177/0022034511431251 ↗
36. Microtensile bond strength and interfacial properties of self-etching and self-adhesive resin cements used to lute composite onlays under different seating forces
37. Bond strength evaluation of three self-adhesive luting systems used for cementing composite and porcelain10.2341/10-205-L ↗
38. Measurement of the microhardness and young’s modulus of human enamel and dentine using an indentation technique10.1016/0003-9969(96)00020-9 ↗
39. Bonding of an auto-adhesive luting material to enamel and dentin10.1016/j.dental.2004.03.002 ↗
40. Microtensile bond strength and scanning electron microscopic evaluation of zirconia bonded to dentin using two self-adhesive resin cements; effect of airborne abrasion and aging10.1016/j.fdj.2017.07.002 ↗
41. Direct comparison of the bond strength results of the different test methods: A critical literature review10.1016/j.dental.2009.12.002 ↗
42. Effect of indirect composite treatment micro effect of indirect composite treatment microtensile bond strength of self-adhesive resin cements
43. Effect of different adhesive strategies on microtensile bond strength of computer aided design/computer aided manufacturing blocks bonded to dentin10.4103/1735-3327.178196 ↗
44. Shear Bond Strength of Indirect Composites Luted with Three New Self-Adhesive Resin Cements to Dentin10.1080/00218460903307779 ↗
45. The shear bond strength of self-adhesive resin cements to dentin and enamel: An in vitro study10.1016/j.prosdent.2014.08.008 ↗
46. Resin cement selection for different types of fixed partial coverage restorations: A narrative systematic review10.1002/cre2.761 ↗
47. The effect of sandblasting duration on the bond durability of dual-cure adhesive cement to CAD/CAM resin restoratives10.4047/jap.2018.10.3.211 ↗
48. The influence of ceramic surface treatments on the tensile bond strength of composite resin to all-ceramic coping materials10.1016/j.prosdent.2005.08.012 ↗
49. Microtensile bond strength between self-adhesive resin cements and resin based ceramic CAD/CAM block
50. Assessment of in vitro methods used to promote adhesive interface degradation: A critical review10.1111/j.1708-8240.2007.00134.x ↗
51. Bond strength of a new universal self-adhesive resin luting cement to dentin and enamel10.1007/s00784-005-0308-5 ↗