Background: Although there are a few studies which compare fast and slow sintering in normal zirconia crowns, it is essential to compare the cracks and load-bearing capacity in zirconia screw-retained implant crowns between regular and speed sintering protocols. This research aimed to compare the surface structure, cracks, and load-bearing capacity in zirconia screw-retained implant crowns between regular sintering (RS) and speed sintering (SS) protocol with and without cyclic loading (fatigue). Methods: A total of 60 screw-retained crowns were fabricated from zirconia (Katana STML Block) by the CAD/CAM system. Then, 30 crowns were subjected to the RS protocol and 30 crowns were subjected to the SS protocol. Cyclic loading was done in half zirconia crowns (15 crowns in each group) using a chewing simulator CS-4.8/CS-4.4 at room temperature. The loading force was applied on the middle of the crowns by a metal stylus underwater at room temperature with a chewing simulator at an axial 50 N load for 240,000 cycles and lateral movement at 2 mm. Scanning electron microscopy was done to study the surface of the crowns and the cracks in the crowns of the regular and speed sintering protocols, with and without fatigue. Results: For the speed sintering group, the surface looks more uniform, and the crack lines are present at a short distance compared to regular sintering. The sintering protocol with a larger Weibull module and durability increases the reliability. It showed that the Speed group showed the maximum fracture load, followed by the regular, speed fatigue, and regular fatigue groups. The fracture load in various groups showed significant differences. Conclusions: It was found that the speed group showed the maximum fracture load followed by the regular, speed fatigue, and regular fatigue. The crack lines ran from occlusal to bottoms (gingiva) and the arrest lines were perpendicular to the crack propagations.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Dental Implant Techniques and Outcomes · Dental materials and restorations · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Prosthetic Dentistry, Faculty of Dentistry, Prince of Songkla University, Hat Yai 90110, Songkhla, Thailand
Funding
Maxillofacial Prosthodontics and Dental Materials Research Unit, Faculty of Dentistry, Prince of Songkla University · Scholarship Award of Thai Ph.D. Student under Thailand’s Education Hub for Southern Region of ASEAN countries
References (39)
Show source-provided references
1. Impact of the material and sintering protocol, layer thickness, and thermomechanical aging on the two-body wear and fracture load of 4y-tzp crowns10.1007/s00784-022-04616-5 ↗
2. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
3. Jung, S., Moser, M.M., Kleinheinz, J., and Happe, A. (2021). Biocompatibility of lithium disilicate and zirconium oxide ceramics with different surface topographies for dental implant abutments. Int. J. Mol. Sci., 22.10.3390/ijms22147700 ↗
4. Abhay, S.S., Ganapathy, D., Veeraiyan, D.N., Ariga, P., Heboyan, A., Amornvit, P., Rokaya, D., and Srimaneepong, V. (2021). Wear resistance, color stability and displacement resistance of milled peek crowns compared to zirconia crowns under stimulated chewing and high-performance aging. Polymers, 13.10.3390/polym13213761 ↗
5. Kongkiatkamon, S., Booranasophone, K., Tongtaksin, A., Kiatthanakorn, V., and Rokaya, D. (2021). Comparison of fracture load of the four translucent zirconia crowns. Molecules, 26.10.3390/molecules26175308 ↗
6. In vitro microscopic evaluation of metal-and zirconium- oxide-based crowns’ marginal fit10.1590/pboci.2022.010 ↗
7. 10-year randomized trial (rct) of zirconia-ceramic and metal-ceramic fixed dental prostheses10.1016/j.jdent.2018.05.015 ↗
8. Heboyan, A., Manrikyan, M., Zafar, M.S., Rokaya, D., Nushikyan, R., Vardanyan, I., Vardanyan, A., and Khurshid, Z. (2021). Bacteriological evaluation of gingival crevicular fluid in teeth restored using fixed dental prostheses: An in vivo study. Int. J. Mol. Sci., 22.10.3390/ijms22115463 ↗
9. Cytotoxicity and biocompatibility of zirconia (y-tzp) posts with various dental cements10.5395/rde.2016.41.3.167 ↗
10. Full digital workflow in the esthetic dental restoration
11. Integrating digital technologies in dentistry to enhance the clinical success
12. Rationale for the use of cad/cam technology in implant prosthodontics10.1155/2013/768121 ↗
13. Chaughule, R.S., and Dashaputra, R. (2021). Applications of cad/cam technology in dental implant planning and implant surgery. Advances in Dental Implantology Using Nanomaterials and Allied Technology Applications, Springer International Publishing.10.1007/978-3-030-52207-0 ↗
14. Jana, S., and Jana, S. (2022). 3d-printed biomaterials in biomedical application. Functional Biomaterials: Drug Delivery and Biomedical Applications, Springer.10.1007/978-981-16-7152-4 ↗
15. Elraggal, A., Aboushelib, M., Abdel Raheem, I.M., and Afifi, R.R. (2022). Effect of surface treatments on biaxial flexural strength, fatigue resistance, and fracture toughness of high versus low translucency zirconia. BMC Oral Health, 22.10.1186/s12903-022-02431-8 ↗
16. Strength, toughness and aging stability of highly-translucent y-tzp ceramics for dental restorations10.1016/j.dental.2016.09.025 ↗
17. Translucency of ips e.Max and cubic zirconia monolithic crowns10.1016/j.prosdent.2017.09.007 ↗
18. Comparison of the mechanical properties of translucent zirconia and lithium disilicate10.1016/j.prosdent.2017.08.004 ↗
19. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗
20. Strength characterization and lifetime prediction of dental ceramic materials10.1016/j.dental.2020.10.015 ↗
21. The effect of surface grinding and sandblasting on flexural strength and reliability of y-tzp zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
22. Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic10.1016/j.dental.2004.07.010 ↗
23. Towards long lasting zirconia-based composites for dental implants: Transformation induced plasticity and its consequence on ceramic reliability10.1016/j.actbio.2016.11.040 ↗
24. Graded ultra-translucent zirconia (5y-psz) for strength and functionalities10.1177/0022034518771287 ↗
25. McLaren, E.A., Maharishi, A., and White, S.N. (2021). Influence of yttria content and surface treatment on the strength of translucent zirconia materials. J. Prosthet. Dent., in press.
26. Fracture strength of implant-supported ceramic crowns with customized zirconia abutments: Screw retained vs. Cement retained10.1111/jopr.12278 ↗
27. Crystallographic and morphological analysis of sandblasted highly translucent dental zirconia10.1016/j.dental.2017.12.008 ↗
28. Kongkiatkamon, S., and Peampring, C. (2022). Effect of speed sintering on low temperature degradation and biaxial flexural strength of 5y-tzp zirconia. Molecules, 27.10.3390/molecules27165272 ↗
29. A fractographic study of clinically retrieved zirconia-ceramic and metal-ceramic fixed dental prostheses10.1016/j.dental.2015.07.003 ↗
30. (2015). Dentistry–Ceramic Materials. Standard No. ISO 6872:2015.
31. A statistical distribution function of wideapplicability10.1115/1.4010337 ↗
32. Nemeth, N.N., Gyekenyesi, J.P., and Jadaan, O.J. (2005). Lifetime Reliability Prediction of Ceramic Structures under Transient Thermomechanical Loads, NASA Center for Aerospace Information.
33. Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
34. Impact of high-speed sintering of three-unit 3y-tzp and 4y-tzp fixed dental prostheses on fracture load with and without artificial aging10.11607/ijp.6775 ↗
35. Impact of high-speed sintering, layer thickness and artificial aging on the fracture load and two-body wear of zirconia crowns10.1016/j.dental.2020.04.004 ↗
36. Effect of high-speed sintering on the flexural strength of hydrothermal and thermo-mechanically aged zirconia materials10.1016/j.dental.2020.05.013 ↗
37. Mechanical behavior and microstructural characterization of different zirconia polycrystals in different thicknesses10.4047/jap.2021.13.6.385 ↗
38. Ordoñez Balladares, A., Abad-Coronel, C., Ramos, J.C., and Martín Biedma, B.J. (2022). Fracture resistance of sintered monolithic zirconia dioxide in different thermal units. Materials, 15.10.3390/ma15072478 ↗
39. Monolithic zirconia crowns: Effect of thickness reduction on fatigue behavior and failure load10.4047/jap.2021.13.5.269 ↗