Fretting and Fretting Corrosion Behavior of Additively Manufactured Ti-6Al-4V and Ti-Nb-Zr Alloys in Air and Physiological Solutions
Source abstract
Abstract
Additive manufacturing (AM) of orthopedic implants has increased in recent years, providing benefits to surgeons, patients, and implant companies. Both traditional and new titanium alloys are under consideration for AM-manufactured implants. However, concerns remain about their wear and corrosion (tribocorrosion) performance. In this study, the effects of fretting corrosion were investigated on AM Ti-29Nb-21Zr (pre-alloyed and admixed) and AM Ti-6Al-4V with 1% nano yttria-stabilized zirconia (nYSZ). Low cycle (100 cycles, 3 Hz, 100 mN) fretting and fretting corrosion (potentiostatic, 0 V vs. Ag/AgCl) methods were used to compare these AM alloys to traditionally manufactured AM Ti-6Al-4V. Alloy and admixture surfaces were subjected to (1) fretting in the air (i.e., small-scale reciprocal sliding) and (2) fretting corrosion in phosphate-buffered saline (PBS) using a single diamond asperity (17 µm radius). Wear track depth measurements, fretting currents and scanning electron microscopy/energy dispersive spectroscopy (SEM/EDS) analysis of oxide debris revealed that pre-alloyed AM Ti-29Nb-21Zr generally had greater wear depths after 100 cycles (4.67 +/− 0.55 µm dry and 5.78 +/− 0.83 µm in solution) and higher fretting currents (0.58 +/− 0.07 µA). A correlation (R2 = 0.67) was found between wear depth and the average fretting currents with different alloys located in different regions of the relationship. No statistically significant differences were observed in wear depth between in-air and in-PBS tests. However, significantly higher amounts of oxygen (measured by oxygen weight % by EDS analysis of the debris) were embedded within the wear track for tests performed in PBS compared to air for all samples except the ad-mixed Ti-29Nb-21Zr (p = 0.21). For traditional and AM Ti-6Al-4V, the wear track depths (dry fretting: 2.90 +/− 0.32 µm vs. 2.51 +/− 0.51 μm, respectively; fretting corrosion: 2.09 +/− 0.59 μm vs. 1.16 +/− 0.79 μm, respectively) and fretting current measurements (0.37 +/− 0.05 μA vs. 0.34 +/− 0.05 μA, respectively) showed no significant differences. The dominant wear deformation process was plastic deformation followed by cyclic extrusion of plate-like wear debris at the end of the stroke, resulting in ribbon-like extruded material for all alloys. While previous work documented improved corrosion resistance of Ti-29Nb-21Zr in simulated inflammatory solutions over Ti-6Al-4V, this work does not show similar improvements in the relative fretting corrosion resistance of these alloys compared to Ti-6Al-4V.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Titanium Alloys Microstructure and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Clemson—Medical University of South Carolina Bioengineering Program, Department of Bioengineering, Clemson University, Charleston, SC 29464, USA
Funding
Wyss Endowment at Clemson University · DePuy Synthes · MUSC T32 Dental Training Grant
References (75)
Show source-provided references
1. In Vitro Corrosion Testing of Titanium Surgical Implant Alloys: An Approach to Understanding Titanium Release from Implants10.1002/jbm.820130206 ↗
2. Textor, M., Sittig, C., Frauchiger, V., Tosatti, S., and Brunette, D.M. (2001). Titanium in Medicine, Springer.
3. Electrochemical impedance spectroscopy study of the passive oxide film on titanium for implant application10.1016/0013-4686(95)00465-3 ↗
4. Electrochemical and XPS studies of titanium for biomaterial applications with respect to the effect of hydrogen peroxide10.1002/jbm.820280115 ↗
5. Okazaki, Y. (2019). Characterization of oxide film of implantable metals by electrochemical impedance spectroscopy. Materials, 12.10.3390/ma12213466 ↗
6. Tribocorrosion behavior of additive manufactured Ti-6Al-4V biomedical alloy10.1016/j.triboint.2017.11.032 ↗
7. Triboelectrochemical techniques and interpretation methods in tribocorrosion: A comparative evaluation10.1016/j.triboint.2007.11.003 ↗
8. Wear-accelerated corrosion of passive metals in tribocorrosion systems10.1149/1.1838341 ↗
9. Tribocorrosion response of the Ti-6Al-4V alloys commonly used in femoral stems10.1016/j.triboint.2013.09.022 ↗
10. Influence of fretting regimes on the tribocorrosion behaviour of Ti-6Al-4V in 0.9wt.% sodium chloride solution10.1016/j.wear.2003.11.003 ↗
11. Significance of Tribocorrosion in Biomedical Applications: Overview and Current Status10.1155/2009/250986 ↗
12. Corrosion and tribocorrosion behaviour of Ti-6Al-4V produced by selective laser melting and hot pressing in comparison with the commercial alloy
13. In vivo severe corrosion and hydrogen embrittlement of retrieved modular body titanium alloy hip-implants10.1002/jbm.b.31171 ↗
14. In vivo oxide-induced stress corrosion cracking of Ti-6Al-4V in a neck–stem modular taper: Emergent behavior in a new mechanism of in vivo corrosion10.1002/jbm.b.31943 ↗
15. Corrosion in the Human Body: Metallic Implants in the Complex Body Environment10.5006/2563 ↗
16. In vivo corrosion of modular hip prosthesis components in mixed and similar metal combinations. The effect of crevice, stress, motion, and alloy coupling10.1002/jbm.820271210 ↗
17. Gilbert, J.L., and Jacobs, J.J. (1997). The Mechanical and Electrochemical Processes Associated with Taper Fretting Crevice Corrosion: A Review, ASTM International.10.1520/STP12020S ↗
18. Mechanically assisted crevice corrosion in metallic biomaterials: A review10.1080/10667857.2016.1223909 ↗
19. In vivo wear of Ti6A14V femoral heads: A retrieval study10.1002/(SICI)1097-4636(199611)32:3<447::AID-JBM19>3.0.CO;2-D ↗
20. Titanium alloys in total joint replacement—A materials science perspective10.1016/S0142-9612(97)00146-4 ↗
21. Friction and wear properties of polymer, metal, and ceramic prosthetic joint materials evaluated on a multichannel screening device10.1002/jbm.820150503 ↗
22. Wear in Total Hip Prostheses: An Experimental Evaluation of Candidate Materials10.3109/ort.1972.43.suppl-145.01 ↗
23. Black staining around titanium alloy prostheses—An orthopaedic enigma10.1302/0301-620X.73B4.2071632 ↗
24. Particulate metallic debris in cemented total hip arthroplasty10.1097/00003086-199308000-00021 ↗
25. Aseptic loosening in total hip arthroplasty secondary to osteolysis induced by wear debris from titanium-alloy modular femoral heads
26. Wear-accelerated corrosion of Ti-6Al-4V and nitrogen-ion-implanted Ti-6Al-4V: Mechanisms and influence of fixed-stress magnitude10.1002/jbm.820210309 ↗
27. Metallosis associated with a stable titanium-alloy femoral component in total hip replacement: A case report
28. Metallic wear in failed titanium-alloy total hip replacements. A histological and quantitative analysis
29. Aluminum: Impacts and Disease10.1006/enrs.2002.4352 ↗
30. Vanadium ionic species from degradation of Ti-6Al-4V metallic implants: In vitro cytotoxicity and speciation evaluation10.1016/j.msec.2018.11.090 ↗
31. The Effect of Hydrogen Peroxide on the Electrochemical Behaviour of Ti-13Nb-13Zr Alloy in Hanks’ Solution10.1590/S1516-14392006000400014 ↗
32. Nanocomposite hydroxyapatite formation on a Ti–13Nb–13Zr alloy exposed in a MEM cell culture medium and the effect of H2O2 addition10.1016/j.actbio.2008.08.008 ↗
33. Microstructural aspects of Ti6Al4V degradation in H2O2-containing phosphate buffered saline10.1016/j.corsci.2021.109640 ↗
34. Corrosion of titanium under simulated inflammation conditions: Clinical context and in vitro investi-gations10.1016/j.actbio.2021.10.002 ↗
35. Wear and corrosion behaviour of Ti-13Nv-13Zr and Ti-6Al-4V alloys in simulated physiological solution10.1016/j.corsci.2010.11.014 ↗
36. Tribological Behaviour of Orthopaedic Ti-13Nb-13Zr and Ti-6Al-4V Alloys10.1007/s11249-010-9639-8 ↗
37. Design of a low Young’s modulus Ti-Zr-Nb-Sn biocompatible alloy by in situ laser powder bed fusion additive manufacturing process10.1016/j.jallcom.2023.171539 ↗
38. Effect of grain size on the recovery strain in a new Ti-20Zr-12Nb-2Sn superelastic alloy10.1016/j.msea.2020.139878 ↗
39. Additive manufacturing of Ti6Al4V alloy via electron beam melting for the development of implants for the biomedical industry10.1016/j.heliyon.2021.e06892 ↗
40. Ben-Shlomo, Y., Blom, A., Boulton, C., Brittain, R., Clark, E., Craig, R., Dawson-Bowling, S., Dere, K., Elsler, C., and Goldberg, A. (2020). The NJR 16th Annual Report 2019, National Joint Registry.
41. Additively manufactured 3D porous Ti-6Al-4V constructs mimic trabecular bone structure and regulate osteoblast proliferation, differentiation and local factor production in a porosity and surface roughness dependent manner10.1088/1758-5082/6/4/045007 ↗
42. Microstructure and mechanical behavior of porous Ti–6Al–4V parts obtained by selective laser melting10.1016/j.jmbbm.2013.05.011 ↗
43. Mechanical evaluation of porous titanium (Ti6Al4V) structures with electron beam melting (EBM)10.1016/j.jmbbm.2009.10.006 ↗
44. Long-term implant fixation and stress-shielding in total hip replacement10.1016/j.jbiomech.2014.12.021 ↗
45. Biomaterials in orthopaedics10.1098/rsif.2008.0151 ↗
46. Excellent mid-term follow-up for a new 3D-printed cementless total knee arthroplasty10.1302/0301-620X.103B6.BJJ-2020-2096.R1 ↗
47. A new 3D printing porous trabecular titanium metal acetabular cup for primary total hip arthroplasty: A minimum 2-year follow-up of 92 consecutive patients
48. Outcomes of novel 3D-printed fully porous titanium cup and a cemented highly cross-linked polyethylene liner in complex and revision total hip arthroplasty10.1186/s42836-022-00152-5 ↗
49. Additively manufactured Ti-29Nb-21Zr shows improved oxide polarization resistance versus Ti-6Al-4V in inflammatory simulating solution10.1002/jbm.a.37552 ↗
50. Fatigue per-formance of zirconia-reinforced Ti-6Al-4V nanocomposite processed by laser powder bed fusion: An improvement by hot isostatic pressing10.1016/j.ijfatigue.2022.107129 ↗
51. Effect of nano-yttria stabilized zirconia addition on the microstructure and mechanical properties of Ti6Al4V parts manufactured by selective laser melting10.1016/j.matdes.2019.107909 ↗
52. Effect of hot isostatic pressing on microstructure and mechanical properties of Ti6Al4V-zirconia nanocomposites processed by laser-powder bed fusion10.1016/j.matdes.2022.110392 ↗
53. Micro-asperity tribocorrosion of CoCrMo, Ti6Al4V, and 316 stainless steel in air and physiological solution: Small scale reciprocal sliding of a single diamond tip10.1016/j.wear.2022.204332 ↗
54. Electrochemical response of CoCrMo to high-speed fracture of its metal oxide using an electro-chemical scratch test method10.1002/(SICI)1097-4636(19971205)37:3<421::AID-JBM13>3.0.CO;2-E ↗
55. Oxygen Diffusion Hardening of Ti-Nb-Zr Alloys10.1080/10426919608947472 ↗
56. Mishra, A.K., Davidson, J.A., Poggie, R.A., Kovacs, P., and FitzGerald, T.J. (1996). Mechanical and Tribological Properties and Biocompatiblity of Diffusion Hardened Ti-13Nb-13Zr—A New Titanium Alloy for Surgical Implants in Medical Applications of Titanium and Its Alloys: The Material and Biological Issues. ASTM Int., 96–113.10.1520/STP16073S ↗
57. Fretting corrosion of CoCrMo and Ti-6Al-4V interfaces10.1016/j.biomaterials.2012.04.015 ↗
58. Li, Z. (2023, December 12). Fretting Corrosion of CoCrMo Alloy Biomaterials: Instrumentation Development, Heredity Integral Modelling and the Effect of Frequency. Available online: https://surface.syr.edu/etd/476.
59. Mace, A., and Gilbert, J.L. (2022). A mass balance analysis of the tribocorrosion process of titanium alloy using a single micro-asperity: Voltage and solution effects on plastic deformation, oxide repassivation, and ion dissolution. J. Mech. Behav. Biomed. Mater., 136.10.1016/j.jmbbm.2022.105531 ↗
60. In situ fabrication of a titanium-niobium alloy with tailored microstructures, enhanced mechanical properties and biocompatibility by using selective laser melting10.1016/j.msec.2020.110784 ↗
61. Selective laser melting of titanium alloy with 50 wt% tantalum: Microstructure and mechanical properties10.1016/j.jallcom.2015.11.141 ↗
62. Early Tibial Component Fractures in Cementless, 3D-Printed, Titanium Implant10.1016/j.artd.2022.08.002 ↗
63. Alpha-case Formation in Ti–6Al–4V in a Different Oxidizing Environment and Its Effect on Tensile and Fatigue Crack Growth Behavior10.1007/s11085-021-10079-y ↗
64. Muthaiah, V.S., Indrakumar, S., Suwas, S., and Chatterjee, K. (2021). Surface engineering of additively manufactured titanium alloys for enhanced clinical performance of biomedical implants: A review of recent developments. Bioprinting, 25.10.1016/j.bprint.2021.e00180 ↗
65. A survey of additive manufacturing trends for FDA-cleared medical devices10.1038/s44222-023-00109-6 ↗
66. Mid-term outcomes of the R3TM delta ceramic acetabular system in total hip arthroplasty10.1186/s13018-020-02192-6 ↗
67. Clinical and hip simulator comparisons of ceramic-on-polyethylene and metal-on-polyethylene wear10.1097/00003086-200010000-00006 ↗
68. Ceramic Heads Decrease Metal Release Caused by Head-taper Fretting and Corrosion10.1007/s11999-015-4683-1 ↗
69. Do ceramic femoral heads reduce taper fretting corrosion in hip arthroplasty? A retrieval study10.1007/s11999-013-3096-2 ↗
70. Mixed-metal fretting corrosion of Ti6Al4V and wrought cobalt alloy10.1002/jbm.820290712 ↗
71. Fretting corrosion of Si3N4 vs. CoCrMo femoral heads on Ti-6Al-V trunnions10.1002/jor.24681 ↗
72. Fretting corrosion of cobalt and titanium implant alloys in simulated body fluids10.5604/01.3001.0010.6922 ↗
73. Cementless Total HIP Arthroplasty Using Biolox® Delta Ceram-ic-on-Ceramic Bearing in Patients with Osteonecrosis of the Femoral Head10.5301/hipint.5000311 ↗
74. Obaton, A.F., Fain, J., Meinel, D., Tsamos, A., Leonard, F., Lecuelle, B., and Djemai, M. (2023). In Vivo Bone Progression in and around Lattice Implants Additvely Manufactured with a New Titanium Alloy. Appl. Sci., 13.10.20944/preprints202305.1280.v1 ↗
75. Kurtz, M.A., Alaniz, K., Kurtz, P.W., Wessinger, A.C., Moreno-Reyes, A., and Gilbert, J.L. (2023). Oxide degradation precedes additively manufactured Ti-6Al-4V selective dissolution: An unsupervised machine learning correlation of impedance and dissolution compared to Ti-29Nb-21Zr. J. Biomed. Mater. Res. Part A, 1–15.10.1002/jbm.a.37632 ↗