Degradable Pure Magnesium Used as a Barrier Film for Oral Bone Regeneration
Source abstract
Abstract
The barrier membrane plays an extremely critical role in guided bone regeneration (GBR), which determines the success or failure of GBR technology. In order to obtain barrier membranes with high mechanical strength and degradability, some researchers have focused on degradable magnesium alloys. However, the degradation rate of pure Mg-based materials in body fluids is rather fast, thus posing an urgent problem to be solved in oral clinics. In this study, a novel micro-arc oxidation (MAO) surface-treated pure Mg membrane was prepared. Electrochemical tests, immersion experiments and in vivo experiments were carried out to investigate its potential use as a barrier membrane. The experimental results showed that the corrosion resistance of a pure Mg membrane treated by MAO is better than that of the uncoated pure Mg. The results of cell experiments showed no obvious cytotoxicity, which suggests the enhanced differentiation of osteoblasts. At the same time, the MAO-Mg membrane showed better biological activity than the pure Ti membrane in the early stage of implantation, exhibiting relatively good bone regeneration ability. Consequently, the MAO membrane has been proven to possess good application prospects for guided bone regeneration.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Bone Tissue Engineering Materials · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Stomatology, The Affiliated Xinhua Hospital of Dalian University, Dalian 116000, China
Key Laboratory of Materials Surface Science and Technology of Jiangsu Province, Changzhou University, Changzhou 213164, China
Mechanical Engineering Department, School of Engineering and Technology, Federal Polytechnic, Offa P.M.B 420, Nigeria
Funding
National Natural Science Foundation of China
References (45)
Show source-provided references
1. Guided bone regeneration (GBR) using membranes and calcium sulphate after apicectomy: A comparative histomorphometrical study10.1046/j.1365-2591.2002.00473.x ↗
2. Guided Bone Regeneration Around Endosseous Implants With Anorganic Bovine Bone Mineral. A Randomized Controlled Trial Comparing Bioabsorbable Versus Non-Resorbable Barriers10.1902/jop.2000.71.11.1743 ↗
3. Current barrier membranes: Titanium mesh and other membranes for guided bone regeneration in dental applications10.1016/j.jpor.2012.12.001 ↗
4. Custom-made titanium devices as membranes for bone augmentation in implant treatment: Clinical application and the comparison with conventional titanium mesh10.1016/j.jcms.2015.10.020 ↗
5. Performances Analysis of Titanium Prostheses Manufactured by Superplastic Forming and Incremental Forming10.1016/j.proeng.2017.04.057 ↗
6. Evaluation of a new bioresorbable barrier to facilitate guided bone regeneration around exposed implant threads. An experimental study in the monkey
7. Biodegradable metals10.1016/j.mser.2014.01.001 ↗
8. A Possible Biodegradable Magnesium Implant Material10.1002/adem.200600252 ↗
9. Lin, D.J., Hung, F.Y., Lee, H.P., and Yeh, M.L. (2017). Development of a Novel Degradation-Controlled Magnesium-Based Regeneration Membrane for Future Guided Bone Regeneration (GBR) Therapy. Metals, 7.10.3390/met7110481 ↗
10. Biocompatibility and Efficiency of Biodegradable Magnesium-Based Plates and Screws in the Facial Fracture Model of Beagles10.1016/j.joms.2018.01.015 ↗
11. Biodegradable magnesium barrier membrane used for guided bone regeneration in dental surgery
12. Characterization and degradation behavior of AZ31 alloy surface modified by bone-like hydroxyapatite for implant applications10.1016/j.apsusc.2008.09.078 ↗
13. Wu, S., Jang, Y.-S., Kim, Y.-K., Kim, S.-Y., Ko, S.-O., and Lee, M.-H. (2019). Surface Modification of Pure Magnesium Mesh for Guided Bone Regeneration: In Vivo Evaluation of Rat Calvarial Defect. Materials, 12.10.3390/ma12172684 ↗
14. In vitro degradation and antibacterial property of a copper-containing micro-arc oxidation coating on Mg-2Zn-1Gd-0.5Zr alloy10.1016/j.colsurfb.2019.03.023 ↗
15. The use of Al–Al2O3 cold spray coatings to improve the surface properties of magnesium alloys10.1016/j.surfcoat.2009.07.032 ↗
16. Biodegradable magnesium fixation screw for barrier membranes used in guided bone regeneration
17. Electroless nickel plating on AZ91 Mg alloy substrate10.1016/j.surfcoat.2005.05.023 ↗
18. Surface Modification on Biodegradable Magnesium Alloys as Orthopedic Implant Materials to Improve the Bio-adaptability: A Review10.1016/j.jmst.2016.05.003 ↗
19. Improvement of corrosion properties of microarc oxidation coating on magnesium alloy by optimizing current density parameters10.1016/j.apsusc.2007.02.010 ↗
20. Comparative study of the effects of MAO coating and Ca-P coating on the biodegradation and biocompatibility of Mg69Zn27Ca4 metal glass
21. Chen, J., Xu, Y., Kolawole, S.K., Wang, J., Su, X., Tan, L., and Yang, K. (2022). Systems, Properties, Surface Modification and Applications of Biodegradable Magnesium-Based Alloys: A Review. Materials, 15.10.3390/ma15145031 ↗
22. Micro-arc oxidation-assisted sol-gel preparation of calcium metaphosphate coatings on magnesium alloys for bone repair10.1016/j.msec.2021.112491 ↗
23. Degradation and biological properties of Ca-P contained micro-arc oxidation self-sealing coating on pure magnesium for bone fixation10.1093/rb/rbu014 ↗
24. Barbeck, M., Kuhnel, L., Witte, F., Pissarek, J., Precht, C., Xiong, X., Krastev, R., Wegner, N., Walther, F., and Jung, O. (2020). Degradation, Bone Regeneration and Tissue Response of an Innovative Volume Stable Magnesium-Supported GBR/GTR Barrier Membrane. Int. J. Mol. Sci., 21.10.3390/ijms21093098 ↗
25. Jung, O., Hesse, B., Stojanovic, S., Seim, C., Weitkamp, T., Batinic, M., Goerke, O., Kacarevic, Z.P., Rider, P., and Najman, S. (2021). Biocompatibility Analyses of HF-Passivated Magnesium Screws for Guided Bone Regeneration (GBR). Int. J. Mol. Sci., 22.10.3390/ijms222212567 ↗
26. The Bioresorption and Guided Bone Regeneration of Absorbable Hydroxyapatite-Coated Magnesium Mesh10.1097/SCS.0000000000003383 ↗
27. Steigmann, L., Jung, O., Kieferle, W., Stojanovic, S., Proehl, A., Gorke, O., Emmert, S., Najman, S., Barbeck, M., and Rothamel, D. (2020). Biocompatibility and Immune Response of a Newly Developed Volume-Stable Magnesium-Based Barrier Membrane in Combination with a PVD Coating for Guided Bone Regeneration (GBR). Biomedicines, 8.10.3390/biomedicines8120636 ↗
28. Effect of flapless ridge preservation with two different alloplastic materials in sockets with buccal dehiscence defects-volumetric and linear changes10.1007/s00784-017-2309-6 ↗
29. Influence of blinded wound closure on the volume stability of different GBR materials: An in vitro cone-beam computed tomographic examination10.1111/clr.12590 ↗
30. Biomechanical Properties of a Novel Biodegradable Magnesium-Based Interference Screw
31. A review on in vitro corrosion performance test of biodegradable metallic materials10.1016/S1003-6326(13)62730-2 ↗
32. Feasibility and Efficacy of a Degradable Magnesium-Alloy GBR Membrane for Bone Augmentation in a Distal Bone-Defect Model in Beagle Dogs10.1155/2022/4941635 ↗
33. Microstructure-modified biodegradable magnesium alloy for promoting cytocompatibility and wound healing in vitro10.1007/s10856-015-5572-6 ↗
34. Assessment of magnesium-based biomaterials: From bench to clinic10.1039/C9BM00289H ↗
35. Effect of pH on the in vitro corrosion rate of magnesium degradable implant material10.1016/j.msec.2010.04.003 ↗
36. The anodic dissolution of magnesium in chloride and sulphate solutions10.1016/S0010-938X(97)00090-5 ↗
37. Enhanced hydrogen evolution on Mg (OH)2 covered Mg surfaces10.1016/j.electacta.2015.02.079 ↗
38. Biodegradable nasal stents (MgF2-coated Mg–2 wt %Nd alloy)—A long-term in vivo study10.1002/jbm.b.33559 ↗
39. In vitro antibacterial properties of magnesium metal against Escherichia coli, Pseudomonas aeruginosa and Staphylococcus aureus10.1016/j.actbio.2009.10.007 ↗
40. Rider, P., Kacarevic, Z.P., Elad, A., Rothamel, D., Sauer, G., Bornert, F., Windisch, P., Hangyasi, D., Molnar, B., and Hesse, B. (2022). Analysis of a Pure Magnesium Membrane Degradation Process and Its Functionality When Used in a Guided Bone Regeneration Model in Beagle Dogs. Materials, 15.10.3390/ma15093106 ↗
41. In vivo study of a biodegradable orthopedic screw (MgYREZr-alloy) in a rabbit model for up to 12 months10.1177/0885328212472215 ↗
42. Long-term in vivo degradation behaviour and biocompatibility of the magnesium alloy ZEK100 for use as a biodegradable bone implant10.1016/j.actbio.2012.08.028 ↗
43. Influence of Different Surface Machining Treatments of Magnesium-based Resorbable Implants on the Degradation Behavior in Rabbits
44. Understanding Magnesium Corrosion—A Framework for Improved Alloy Performance10.1002/adem.200310405 ↗
45. Comparison of the resorbable magnesium. alloys LAE442 und MgCa0.8 concerning their mechanical properties, their progress of degradation and the bone-implant-contact after 12 months implantation duration in a rabbit model10.1002/mawe.200800412 ↗