The Effect of Hydrogen on the Fracture Properties of 0.8(Na1/2Bi1/2)TiO3-0.2(K1/2Bi1/2)TiO3 Ferroelectric Ceramics

H. Zhang, Y.J. Su, L.J. Qiao, W.Y. Chu, D. Wang, Y.X. Li

Journal of Electronic Materials· Volume 37· Issue 3
Publisher page

Abstract

The effect of hydrogen on the fracture properties of lead-free ferroelectric ceramics has been studied. For hydrogen precharged samples, the fracture toughness decreased linearly with both increasing hydrogen concentration and the logarithm of dwell time of indenting. Hydrogen-induced delayed propagation of unloaded indentation cracks can occur, and the threshold stress intensity factor of hydrogen-induced cracking induced by residual stress decreases linearly with increasing hydrogen concentration.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Hydrogen embrittlement and corrosion behaviors in metals · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. J.P. Han, T.P. Ma, Appl. Phys. Lett. 71, 1267 (1997)10.1063/1.119869 ↗
2. S. Aggarwal, S.R. Perusse, C.W. Tipton, R. Ramesh, N.H. Drew, T. Venkatesan, D.B. Romero, V.B. Podobedov, A. Weber, Appl. Phys. Lett. 73, 1973 (1998)10.1063/1.122339 ↗
3. T. Tamura, K. Matsuura, H. Ashida, K. Kondo, S. Otani, Appl. Phys. Lett. 74 (1999) 339510.1063/1.123356 ↗
4. S. Aggarwal, S.R. Perusse, B. Nagaraj, R. Ramesh, Appl. Phys. Lett. 74, 3023 (1999)10.1063/1.124052 ↗
5. J.T. Evans, L.L. Boyer, G. Velasquez, R. Ramesh, S. Aggavwal, V. Keramidas, Japan J. Appl. Phys. B 389, 5361 (1999)10.1143/JJAP.38.5361 ↗
6. N.R. Rajopadhye, S.S.V. Bhoraskar, A.P.B. Sinha, J. Mater. Sci. 23, 2631 (1999)10.1007/BF01111925 ↗
7. W.P. Chen, L.T. Li, Y. Wang, Z.L. Gui, J. Mater. Res. 13, 1110 (1998)10.1557/JMR.1998.0154 ↗
8. N. Ikarashi, Appl. Phys. Lett. 73, 1955 (1998)10.1063/1.122333 ↗
9. W.P. Chen, H.L.W. Chan, Appl. Phys. Lett. 80, 3587 (2002)10.1063/1.1479205 ↗
10. W.P. Chen, X.P. Jiang, Z. Peng, H.L.W. Chan, J. Am. Ceram. Soc. 86, 735 (2003)10.1111/j.1151-2916.2003.tb03366.x ↗
11. J.S. Hwang, W.S. Kima, H.H. Park, T.S. Kim, Sensor Actuat. A. 117, 137 (2005)10.1016/j.sna.2004.05.033 ↗
12. X. Peng, Y.J. Su, K.W. Gao, L.J. Qiao, W.Y. Chu, Mater. Lett. 58, 2073 (2004)10.1016/j.matlet.2004.01.004 ↗
13. Y. Wang, W.Y. Chu, L.J. Qiao, Y.J. Su, Mater. Sci. Eng. B 98, 1 (2002)10.1016/S0921-5107(02)00395-1 ↗
14. G.R. Anstis, P. Chantikul, B.R. Lawn, D.B. Marshall, J. Am. Ceram. Soc. 64, 533 (1981)10.1111/j.1151-2916.1981.tb10320.x ↗
15. F. Fang, W. Yang, Mater. Lett. 46, 131 (2000)10.1016/S0167-577X(00)00155-5 ↗
16. D.K. Shelly, I.G. Wright, P.N. Mincer, A.H. Clauer, J. Mater. Sci. 20, 1873 (1983)
17. J.P. Hirth, Metall. Trans. A 11, 861 (1980)10.1007/BF02654700 ↗
18. G.P. Cherepanov, Mechanics of Brittle Fracture, McGraw-Hill, New York, 1977, p. 29
19. P. Chantikul, G.R. Anstis, B.R. Laun, D.B. Marshall, J. Am. Ceram. Soc. 64, 539 (1981)10.1111/j.1151-2916.1981.tb10321.x ↗