Piezoelectric and dielectric properties of CeO2-doped (Bi0.5Na0.5)0.94Ba0.06TiO3 lead-free ceramics
Source abstract
Abstract
Abstract CeO 2 -doped (Bi 0.5 Na 0.5 ) 0.94 Ba 0.06 TiO 3 lead-free piezoelectric ceramics (0–1.0 wt.%) were synthesized by conventional solid-state processes. X-ray diffraction (XRD) data shows that CeO 2 diffuses into the lattice of (Bi 0.5 Na 0.5 ) 0.94 Ba 0.06 TiO 3 ceramics and forms pure perovskite phase. SEM images indicate that a small amount of CeO 2 addition affects the microstructure. The electrical properties of (Bi 0.5 Na 0.5 ) 0.94 Ba 0.06 TiO 3 ceramics have been greatly improved by a certain amount of CeO 2 addition. The temperature dependence of the dielectric constant and dissipation factor shows that the transition temperature from ferroelectric to antiferroelectric phase ( T d ) decreases with the addition of CeO 2 . At the room temperature, the ceramics doped with 0.4 wt.% CeO 2 show quite good performance with high piezoelectric constant ( d 33 = 128 pC/N), high planar coupling factor ( k p = 0.283), high mechanical quality factor ( Q m = 216), high thick coupling factor ( k t = 0.54), high dielectric constant ( ɛ r = 891) and low dissipation factor (tan δ = 0.0185) at 1 kHz, which indicates that CeO 2 -doped sample is of high piezoelectric properties and low dissipation factor. Possible mechanism of the influence of CeO 2 addition on the dielectric and piezoelectric properties is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Chiang · Appl. Phys. Lett. · 1998 · 73 · 368310.1063/1.122862 ↗
2. Xiao · Electr. Components Mater. · 2004 · 23 · 62
3. Saito · Nature · 2004 · 432 · 8410.1038/nature03028 ↗
4. Coss · Nature · 2004 · 432 · 2410.1038/nature03142 ↗
5. Smolenskii · Sov. Phys. Solid State · 1961 · 2 · 2651
6. Nagata · J. Eur. Ceram. Soc. · 2001 · 21 · 129910.1016/S0955-2219(01)00005-X ↗
7. Wang · Solid State Commun. · 2004 · 129 · 31910.1016/j.ssc.2003.10.017 ↗
8. Chu · J. Eur. Ceram. Soc. · 2002 · 22 · 211510.1016/S0955-2219(02)00027-4 ↗
9. Sasaki · Jpn. J. Appl. Phys. · 1999 · 38 · 556410.1143/JJAP.38.5564 ↗
10. Elkechai · Phys. Status Solidi · 1996 · 157 · 49910.1002/pssa.2211570234 ↗
11. Li · Mater. Sci. Eng. B · 2004 · 112 · 510.1016/j.mseb.2004.04.019 ↗
12. Wang · J. Am. Ceram. Soc. · 2003 · 86 · 180910.1111/j.1151-2916.2003.tb03562.x ↗
13. Wang · Appl. Phys. Lett. · 2004 · 85 · 9110.1063/1.1767592 ↗
14. Lin · J. Eur. Ceram. Soc. · 2006 · 26 · 324710.1016/j.jeurceramsoc.2005.09.038 ↗
15. Wang · Mater. Lett. · 2007 · 61 · 384710.1016/j.matlet.2006.12.045 ↗
16. Takenaka · Jpn. J. Appl. Phys. · 1991 · 30 · 223610.1143/JJAP.30.2236 ↗
17. Xu · 1978
18. IEEE Standard on Piezoelectricity, IEEE Standard 176-1987, Institute of Electronic Engineers, New York, 1987.
19. Onoe · J. Acoust. Soc. Am. · 1967 · 41 · 97410.1121/1.1910452 ↗
20. Roy-Chowdhury · J. Mater. Sci. (USA) · 1987 · 22 · 220910.1007/BF01132962 ↗
21. Wang · Solid State Commun. · 2003 · 125 · 39510.1016/S0038-1098(02)00816-5 ↗
22. Thomas · J. Phys. Chem. Solid · 1990 · 51 · 141910.1016/0022-3697(90)90025-B ↗