journal article·2015-04

Enhanced ferroelectric properties of (111) oriented Pb(Hf0.3Ti0.7)O3 thin films deposited using self-buffered layer

Y.L. Lin, J. Zhu, Z.P. Wu, W.B. Luo, X.P. Liu, S.J. Wu, L.Z. Hao

Publisher page

Abstract

Abstract Lead hafnate-titanate (PHT) thin films have been prepared via pulsed laser deposition (PLD) on Pt(1 1 1)/Ti/SiO 2 /Si(1 0 0) substrates by inserting a low temperature (200–400 °C) self-buffered layer. It is found that the self-buffered layers deposited at different temperatures have a great influence on the microstructure and electric properties. XRD spectra, including θ –2 θ and ω scans, show that the PHT films with (1 1 1) preferred orientation were successfully deposited on substrates by inserting a low temperature self-buffered layer. Compared with the PHT films directly deposited at a high temperature, the PHT films with an inserted low temperature (300 °C) self-buffered layer have significantly enhanced electrical properties of four orders of magnitude lower leakage current density (3.2 × 10 −8 A/cm 2 at 150 kV/cm), 1.5 times larger remnant polarization (2Pr = 63 μC/cm 2 ), 0.4 times smaller coercive field (2Ec = 190 kV/cm), and more excellent fatigue endurance (almost no degradation after 2 × 10 10 switching cycles). The use of self-buffered layer is an effective approach to fabricate PHT ferroelectric materials with large ferroelectric polarization and long fatigue endurance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Ferroelectric and Negative Capacitance Devices · Multiferroics and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Shim · J. Alloys Comp. · 2008 · 449 · 3210.1016/j.jallcom.2006.02.088 ↗
2. Do · Nat. Mater. · 2004 · 3 · 36510.1038/nmat1122 ↗
3. Tagantsev · J. Appl. Phys. · 2001 · 90 · 138710.1063/1.1381542 ↗
4. Wang · J. Appl. Phys. · 2008 · 104 · 07411210.1063/1.2996080 ↗
5. Pintilie · Appl. Phys. Lett. · 2006 · 88 · 10290810.1063/1.2186074 ↗
6. Verdier · Appl. Phys. Lett. · 2004 · 85 · 321110.1063/1.1801679 ↗
7. Fantozzia · J. Eur. Ceram. Soc. · 2000 · 20 · 167110.1016/S0955-2219(00)00051-0 ↗
8. Frantti · Inorg. Chem. · 2005 · 44 · 926710.1021/ic051169m ↗
9. Schorn · J. Am. Ceram. Soc. · 2005 · 88 · 131210.1111/j.1551-2916.2004.00177.x ↗
10. Kim · Thin Solid Films · 2002 · 416 · 26410.1016/S0040-6090(02)00726-5 ↗
11. Li · Appl. Phys. Lett. · 2004 · 84 · 526110.1063/1.1764944 ↗
12. Pintilie · Appl. Phys. Lett. · 2009 · 94 · 23290210.1063/1.3152784 ↗
13. Kügeler · Appl. Phys. A · 2009 · 94 · 73910.1007/s00339-008-5045-6 ↗
14. Wu · J. Appl. Phys. · 2009 · 105 · 04410710.1063/1.3081971 ↗
15. Xiao · J. Phys. D: Appl. Phys. · 2014 · 47 · 18530310.1088/0022-3727/47/18/185303 ↗
16. Kang · J. Vac. Sci. Technol. A · 2002 · 20 · 149810.1116/1.1488947 ↗
17. Pandey · Mater. Sci. Eng., B · 2004 · 112 · 9610.1016/j.mseb.2004.06.011 ↗
18. Palange · Thin Solid Films · 2003 · 428 · 16010.1016/S0040-6090(02)01168-9 ↗
19. Lu · Thin Solid Films · 1999 · 348 · 3810.1016/S0040-6090(98)01767-2 ↗
20. Ohashi · J. Appl. Phys. · 2002 · 92 · 237810.1063/1.1495530 ↗
21. Shin · Thin Solid Films · 2010 · 518 · 649610.1016/j.tsf.2010.03.148 ↗
22. Hu · J. Mater. Res. · 1994 · 9 · 148410.1557/JMR.1994.1484 ↗
23. Botea · Appl. Phys. Lett. · 2013 · 103 · 23290210.1063/1.4838035 ↗
24. Zhang · J. Alloys Comp. · 2009 · 487 · 70310.1016/j.jallcom.2009.08.049 ↗
25. Aoki · Jpn. J. Appl. Phys., Part 1 · 1995 · 34 · 74610.1143/JJAP.34.746 ↗
26. Yan · Thin Solid Films · 2002 · 406 · 28210.1016/S0040-6090(01)01745-X ↗