Enhanced high-power behaviors of Mn-doped Pb (In1/2Nb1/2) O3-Pb(Mg1/3Nb2/3) O3-PbTiO3 piezoelectric crystals through combining direct and alternating current polarization
Source abstract
Abstract
Elevating both the mechanical quality factor and piezoelectric properties is pivotal for enhancing the efficiency of high-power piezoelectric devices. Mn-doped Pb (In 1/2Nb 1/2) O 3-Pb(Mg1/3Nb2/3) O 3-PbTiO 3 (Mn: PIN-PMN-PT) single crystals have previously exhibited a notable mechanical quality factor, yet encountered a substantial decline in piezoelectric coefficient. In pursuit of the concurrent optimization of these parameters, we explored the co-enhancement of mechanical quality factor and piezoelectric coefficient in [001]-oriented Mn: PIN-PMN-PT single crystals by employing a synergistic approach (DCP-ACP) involving direct-current poling (DCP) and alternating-current poling (ACP). Our investigation reveals a remarkable improvement, with the piezoelectric coefficient and mechanical quality factor experiencing a notable surge of 53% and 118%, respectively, compared to the outcomes achieved with DCP alone. Compared to the ACP method, the piezoelectric coefficient and the mechanical quality factor were improved more than 7% and 18%, respectively. Moreover, the coercive field and remnant polarization of the single crystals witnessed a substantial upswing post DCP-ACP. The results are attributed to the elimination of the 71° domain walls, as observed through polarized light microscopy. Here we demonstrate Mn: PIN-PMN-PT single crystals are expected to has high mechanical quality factor and strong piezoelectric constants through DCP-ACP, thus suggesting a new route to high performance ferroelectrics.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Multiferroics and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Pyroelectric devices and materials10.1088/0034-4885/49/12/002 ↗
2. Ultrahigh strain and piezoelectric behavior in relaxor based ferroelectric single crystals10.1063/1.365983 ↗
3. Advantages and challenges of relaxor-PbTiO3 ferroelectric crystals for electroacoustic transducers – A review10.1016/j.pmatsci.2014.10.002 ↗
4. A two-step annealing method to enhance the pyroelectric properties of Mn: PIMNT chips for infrared detectors10.3390/ma13112562 ↗
5. Enhanced pyroelectric properties and application of tetragonal Mn-doped 0.29Pb(In1/2Nb1/2) O3-0.31Pb(Mg1/3Nb2/3) O3-0.40PbTiO3 ternary single crystals10.1016/j.jallcom.2016.07.314 ↗
6. Excellent ferroelectric and pyroelectric performance of rhombohedral Mn-doped PIMNT thin films with (111) orientation10.1111/jace.18054 ↗
7. Hardening of (Ba0.5Na0.5)0.85Ba0.15TiO3 lead-free piezoelectric ceramics by adding (Bi0.5Na0.5) MnO310.35848/1347-4065/ac564e ↗
8. High mechanical quality factor and piezoelectricity in potassium sodium niobate ceramics10.1016/j.ceramint.2021.11.204 ↗
9. Enhancing electromechanical properties of PZT-based piezoelectric ceramics by high-temperature poling for high-power applications10.1021/acsami.2c19802 ↗
10. Effects of impurities on the mechanical quality factor of lead zirconate titanate ceramics10.1143/JJAP.11.31 ↗
11. Effects of manganese addition on piezoelectric properties of Pb(Zr0.5Ti0.5) O310.1143/JJAP.31.3058 ↗
12. Elastic, dielectric and piezoelectric characterization of single domain PIN-PMN-PT: Mn crystals10.1063/1.4772617 ↗
13. Orientation dependence of piezoelectric properties and mechanical quality factors of 0.27Pb(In1/2Nb1/2) O3-0.46Pb(Mg1/3Nb2/3) O3-0.27PbTiO3: Mn single crystals10.1063/1.4821030 ↗
14. N. Yamamoto, Y. Yamashita, Y. Hosono, et al., Ultrasonic probe, piezoelectric transducer, method of manufacturing ultrasonic probe, and method of manufacturing piezoelectric transducer. Japan. Patent, US13975508, 2014-03-06.
15. Y. Yamashita, N. Yamashita, Y. Hosono, et al., Piezoelectric transducer, ultrasonic probe, and piezoelectric transducer manufacturing method. Japan. Patent. US201500372219A1, 2015-12-24.
16. Enhanced dielectric and piezoelectric properties of manganese-doped Pb(In1/2Nb1/2) O3-Pb(Mg1/3Nb2/3) O3-PbTiO3 single crystals by alternating current poling10.1063/5.0038207 ↗
17. Simultaneous enhancement of piezoelectricity and mechanical quality factor in relaxor-ferroelectric crystals via defect engineering10.1063/5.0141634 ↗
18. Effect of low-frequency alternating current poling on 5-mm-thick 0.7Pb(Mg1/3Nb2/3) O3-0.3PbTiO3 single crystals
19. Impact of alternating current electric field poling on piezoelectric and dielectric properties of Pb(In1/2Nb1/2) O3–Pb(Mg1/3Nb2/3) O3–PbTiO3 ferroelectric crystals.10.1063/5.0020109 ↗
20. Growth and characterization of relaxor ferroelectric PMNT single crystals10.1080/00150199908014518 ↗
21. Compositional homogeneity and electrical properties of lead magnesium niobate titanate single crystals grown by a modified bridgman technique10.1143/JJAP.39.5581 ↗
22. Growth and electrical properties of large size Pb(In1∕2Nb1∕2) O3–Pb(Mg1∕3Nb2∕3) O3–PbTiO3 crystals prepared by the vertical Bridgman technique.
23. Structural quality of relaxor-based ferroelectric [111] oriented Pb(Mg1/3Nb2/3) O3–0.26PbTiO3 single crystals10.1016/j.mseb.2006.06.055 ↗
24. Large electric-field-induced strain in ferroelectric crystals by point-defect-mediated reversible domain switching10.1038/nmat1051 ↗
25. Positive/negative electrocaloric effect induced by defect dipoles in PZT ferroelectric bilayer thin films10.1039/C6RA14776C ↗
26. Giant electromechanical coupling factor of k31 mode in Pb(Zn1/3Nb2/3) O3-PbTiO3 and Pb(Mg1/3Nb2/3) O3-PbTiO3 single crystals10.1080/00150190600737875 ↗
27. Characteristics of relaxor-based piezoelectric single crystals for ultrasonic transducers10.1109/58.655639 ↗
28. Relaxor-PT single crystals: observations and developments10.1109/TUFFC.2010.1670 ↗
29. Dielectric and piezoelectric properties of 0.7 Pb(Mg1/3Nb2/3) O3-0.3 PbTiO3 single crystal poled using alternating current10.1080/21663831.2018.1498812 ↗
30. Enhanced dielectric and piezoelectric properties in the [001]-poled 0.25Pb(In1/2Nb1/2) O3-0.43Pb(Mg1/3Nb2/3) O3-0.32PbTiO3 single crystal near morphotropic phase boundary by alternating current treatment10.1063/1.5126060 ↗
31. The performance enhancement and temperature dependence of piezoelectric properties for Pb(Mg1/3Nb2/3) O3-0.30PbTiO3 single crystal by alternating current polarization
32. Effect of field cooling AC poling on electrical and physical properties for Pb(Mg1/3Nb2/3) O3-PbTiO3-based single crystals manufactured by a continuous-feeding Bridgman process10.35848/1347-4065/abb2fe ↗
33. Enhanced electric property of relaxor ferroelectric crystals with low AC voltage high-temperature poling10.35848/1347-4065/abb2ff ↗
34. Enhanced piezoelectric properties and strain response in [001] textured BNT-BKT-BT ceramics10.1016/j.matdes.2017.10.003 ↗
35. Transparent ferroelectric crystals with ultrahigh piezoelectricity10.1038/s41586-019-1891-y ↗
36. Effect of Mn on dielectric and piezoelectric properties of 71PMN-29PT [71Pb(Mg1/3Nb2/3) O3-29PbTiO3] single crystals and polycrystalline ceramics10.4191/kcers.2018.55.2.04 ↗
37. Elastic, piezoelectric, and dielectric properties of multidomain 0.67Pb(Mg1/3Nb2/3) O3–0.33PbTiO3 single crystals.10.1063/1.1390494 ↗
38. Characterization of Pb(In1/2Nb1/2) O3–Pb(Mg1/3Nb2/3) O3–PbTiO3 ferroelectric crystal with enhanced phase transition temperatures.10.1063/1.2978333 ↗
39. Complete set of material constants of Pb(In1/2Nb1/2) O3-Pb(Mg1/3Nb2/3) O3-PbTiO3 single crystal with morphotropic phase boundary composition
40. Characterization of Mn-doped PIN-PMN-PT single crystal grown by continuous-feeding bridgman method10.3390/cryst12091183 ↗
41. Temperature-dependent phase transition in [001]C-oriented 0.72Pb(Mg1/3Nb2/3) O3-0.28PbTiO3 single crystals10.1016/j.ceramint.2019.04.099 ↗
42. Thermal annealing effects on the energy storage properties of BST ceramics10.1111/jace.14903 ↗
43. Enhanced piezoelectric properties of barium titanate single crystals with different engineered-domain sizes
44. Optimization of piezoelectric properties for [001]c poled 0.94Pb(Zn1/3Nb2/3) O3–0.06PbTiO3 single crystals10.1063/1.3314285 ↗
45. Domain engineering and full matrix material constants of the [111]c-poled 0.63Pb(Mg1/3Nb2/3)-0.37PbTiO3 single crystal10.1039/C8CE00831K ↗
46. Piezoelectric performance enhancement of Pb(Mg1/3Nb2/3) O3-0.25PbTiO3 crystals by alternating current polarization for ultrasonic transducer10.1063/1.5027591 ↗