journal article·2004-10

Chemical mechanical planarization for microelectronics applications

Parshuram B. Zantye, Ashok Kumar, A.K. Sikder

Publisher page

Abstract

Abstract The progressively decreasing feature size of the circuit components has tremendously increased the need for the global surface planarization of the various thin film layers that constitute the integrated circuit (IC). Global planarization, being one of the major solutions to meet the demands of the industry, needs to be achieved following the most efficient polishing procedure. Chemical mechanical polishing (CMP) is the planarization method that has been selected by the semiconductor industry today. CMP, an ancient process used for glass polishing, was adopted first as a microelectronic fabrication process by IBM in the 80 s for SiO2 polishing. To achieve efficient planarization at miniaturized device dimensions, there is a need for a better understanding of the physics, chemistry and the complex interplay of tribo-mechanical phenomena occurring at the interface of the pad and wafer in presence of the fluid slurry medium. In spite of the fact that CMP research has grown by leaps and bounds, there are some teething problems associated with CMP process such as delamination, microscratches, dishing, erosion, corrosion, inefficient post-CMP clean, etc.; research on which is still developing. The fundamental understanding of the CMP is highly necessary to characterize, optimize and model the process. The CMP process is ready to make a positive impact on 30% of the US$ 135 billion global semiconductor market. This paper presents an overview of CMP process in general, the science and mechanism of polishing, different metal and dielectric CMP processes. The impact of consumables on the CMP process, post-CMP cleaning, modeling of different CMP processes as well as the future trends are also discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Integrated Circuits and Semiconductor Failure Analysis · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. The evolution of interconnection technology at IBM10.1147/rd.394.0371 ↗
2. Borst · 2002
3. CMOS scaling into the 21st century: 0.1 μM and beyond10.1147/rd.391.0245 ↗
4. Internet web site: http://www.intel.com/labs/features/si11032.htm, Intel, 2002.
5. A low-temperature local interconnect process in a 0.25 μm channel CMOS logic technology with shallow trench isolation
6. Internet web site: http://www.research.ibm.com/, IBM, 2003.
7. Review of technology for 157 nm lithography10.1147/rd.455.0605 ↗
8. Advanced optical lithography development, from UV to EUV
9. Printing meets lithography: soft approaches to high-resolution patterning10.1147/rd.455.0697 ↗
10. Wolf · 1991
11. Fundamental limits in physical information processing10.1109/PROC.1981.11959 ↗
12. Murarka · 1993
13. Lee · 2003 · F7.4
14. International Technology Roadmap for Semiconductors, 2001.
15. Shenai · 1991
16. Analysis and modeling of multilevel parallel and crossing interconnections lines10.1109/T-ED.1987.22976 ↗
17. Solution of partial differential equations with a resistance network analogue10.1088/0508-3443/1/4/303 ↗
18. Losses on multiconductor transmission lines in multilayered dielectric media10.1109/TMTT.1984.1132757 ↗
19. P. Wolters, Internet web site: http://www.peter-wolters.com/cmp/cmpmultilevel.htm, 2003.
20. An optimization of tungsten plug chemical mechanical polishing (CMP) using different consumables10.1023/A:1011276830620 ↗
21. Application of chemical mechanical polishing to the fabrication of VLSI circuit interconnection10.1149/1.2085872 ↗
22. Wolf · 1991
23. STI process steps for sub-quarter micron CMOS10.1016/S0026-2714(97)00166-2 ↗
24. A study on the reproducibility of HSS STI–CMP process for ULSI applications10.1016/S0167-9317(02)00931-0 ↗
25. An optimized nitride residue phenomena of shallow trench isolation (STI) process by chemical mechanical polishing (CMP)
26. Correlation analysis between pattern and non-pattern wafer for characterization of shallow trench isolation-chemical mechanical polishing (STI–CMP) process10.1016/S0167-9317(01)00694-3 ↗
27. Reduction of process defects using a modified set-up for chemical mechanical polishing equipment
28. Effects of STI-fill thickness on the CMP process defects10.1016/j.mee.2003.11.005 ↗
29. C. Chen, J.-Y. Wu, W. Lur, US Patent 6,169,012 (2001).
30. C. Chen, J.-Y. Wu, W. Lur, US Patent 6,486,040 (2002).
31. C. Chen, J.-Y. Wu, W. Lur, US Patent 6,448,159 (2002).
32. Three-dimensional wafer-scale copper chemical–mechanical planarization model10.1016/S0040-6090(02)00329-2 ↗
33. Fluid pressure and its effects on chemical mechanical polishing10.1016/S0043-1648(02)00155-2 ↗
34. Structural and electronic properties of low dielectric constant carbon rich amorphous silicon carbide10.1016/S0925-9635(02)00220-0 ↗
35. Electrical characterization of copper interconnects with end-of-roadmap feature sizes10.1016/S0038-1101(03)00042-X ↗
36. Dry etch challenges of 0.25 μm dual damascene structures10.1016/S0167-9317(97)00094-4 ↗
37. L. Shon-Roy, Integrated Circuit Engineering Corporation Handbook, 1999.
38. Low polarization and low temperature reflow of inorganic borophosphosilicate glasses formed from organic sources10.1016/S0921-5107(02)00311-2 ↗
39. Relationship between electronic molar polarizability and super low dielectric constant in B2O3–BeF2–C glass systems10.1016/S0022-3697(98)00063-8 ↗
40. Reflow of BeF2, B2O3, GeO2, SiO2 glasses and application of their membranes to metal-oxide-silicon (MOS) capacitors10.1016/0921-5107(96)01554-1 ↗
41. Viscous flow of ZnF2- and Si3N4-containing borosilicate glasses and their applications to MOS capacitors10.1016/S0025-5408(98)00004-X ↗
42. Improvement of polarizable capacitance—voltage curves of MOS capacitors passivated with BN-and PbF2-containing SiO2–B2O3–GeO2 glasses10.1016/S0022-3093(97)00138-5 ↗
43. Levert · 1999
44. Thermomechanical properties and moisture uptake characteristics of hydrogen silsesquioxane submicron films10.1063/1.123417 ↗
45. Open volume defects (measured by positron annihilation spectroscopy) in thin film hydrogen-silsesquioxane spin-on-glass; correlation with dielectric constant10.1063/1.371174 ↗
46. A new study on spin-on-silica for multilevel interconnect applications10.1016/S0026-2692(98)00099-8 ↗
47. Planarization properties of hydrogen silsesquioxane (HSQ) influence on CMP10.1016/S0167-9317(99)00261-0 ↗
48. Changes in material properties of low-k interlayer dielectric polymers induced by exposure to plasmas10.1016/S0167-9317(03)00165-5 ↗
49. C.T. Chua, Y.-P. Lee, M.S. Zhou, L. Chan, US Patent 6,121,130 (2000).
50. A.E. Braun, Low-k integration advances with hesitation, Semicond. Int. 11 May 2003.
51. Köhler · 1999
52. Esashi · Microsyst. Technol. · 1994 · 1 · 210.1007/BF01367754 ↗
53. Anisotropic etching of polycrystalline silicon with hot Cl2 molecular beam10.1063/1.341413 ↗
54. Etching mechanism of vitreous silicon dioxide in HF-based solutions10.1021/ja993803z ↗
55. CMP mechanism identified at Bell Laboratory
56. Steigerwald · 1997
57. Atomic force microscoy, lateral force microscopy, and transmission electron microscopy investigations and adhesion force measurements for elucidation of tungsten removal mechanisms10.1557/JMR.1999.0499 ↗
58. Integration of chemical–mechanical polishing into CMOS integrated circuit manufacturing10.1016/0040-6090(92)90539-N ↗
59. Internet web site: http://www.memc.com/MEMC.nsf/0/6D86FAED316FE14686256AE80058166D/$File/Ultraflat_wafers.pdf?OpenElement, © MEMC, 2003.
60. Internet web site: http://www.komsil.co.jp/en/office/hist.htm, © Komatsu, 2003.
61. Internet web site: http://www.research.ibm.com, © IBM, 2004.
62. Internet web site: http://www.sematech.org/corporate/index.htm, © Sematch Inc., 2004.
63. Internet web site: http://www.mitsubishi.or.jp/e/monitor/monitor_old/97version/monitor9802/wafer.html, © Mitsubishi, 2004.
64. A.K. Sikder, P. Zantye, S. Thagella, A. Kumar, B. Michael Vinogradov, N.V. Gitis, Proceedings of 8th CMPMIC Conference, 2003, p. 120.
65. S.H. Li, R. Miller, Chemical Mechanical Polishing in Silicon Processing, vol. 63, Academic Press, New York, 2000, Semiconduct. Semimet.
66. Chemical mechanical polishing of Al and SiO2 thin films: the role of consumables10.1149/1.1392688 ↗
67. Basim · J. Colloid Interface Sci. · 2002 · 256 · 13710.1006/jcis.2002.8352 ↗
68. Internet web site: http://www.pall.com/catalogs/microelec/cmp, © Pall, 2003.
69. Internet web site: http://www.amat.come, © Applied Materials Inc., 2003.
70. Application of chemical mechanical polishing to the fabrication of VLSI circuit interconnection10.1149/1.2085872 ↗
71. A four-level VLSI bipolar metallization design with chemical–mechanical planarization10.1147/rd.365.0845 ↗
72. Internet web site: http://www.sea.rl.ac.uk/oldsea/oldpubs/Ale/desc.htm, Semiconductor Equipment Assessment, 2002.
73. Pad porosity, compressibility and slurry delivery effects in chemical–mechanical planariztion: modeling and experiments10.1016/S0040-6090(00)00748-3 ↗
74. The effect pf the polishing pad treatment on the chemical–mechanical polishing of SiO2 films10.1016/0040-6090(96)80082-4 ↗
75. CMP CoO reduction: slurry reprocessing
76. Pad conditioning in chemical mechanical polishing10.1016/S0924-0136(01)01137-2 ↗
77. Quantitative analysis of physical and chemical changes in CMP polyurethane pad surfaces10.1016/S1044-5803(02)00285-1 ↗
78. B. Mullany, J. Mater. Process. Technol. 132 (1–3, 10) (2003) 28.10.1016/S0924-0136(02)00205-4 ↗
79. Internet web site: http://www.sfamipec.com/product/polish_sing.html, Speed Fam, 2004.
80. Localized corrosion effects and modifications of acidic and alkaline slurries on copper chemical mechanical polishing10.1016/S0169-4332(02)01224-2 ↗
81. Signal analysis of the end point detection method based on motor current10.1016/S0167-9317(02)00930-9 ↗
82. J.M. Boyd, H.E. Litvak, US Patent 6,612,902 (2003).
83. C.-H. Lu, M.-Y. Li, US Patent 6,307,628 (2002).
84. N. Saka, J. Nam, H.L. Oh, US Patent 6,476,921 (2001).
85. A.K. Sikder, private communication, 2003.10.1016/S0304-3894(02)00169-3 ↗
86. A.K. Sikder, private communication, 2002.
87. F.-S. Lee, C.-C. Chen, J.-C. Lee, H.-C. Huang, US Patent 6,503,124 (2003).
88. T. Shih, C.-H. Yu, US Patent 6,682,396 (2004).
89. S.R. Roy, US Patent 6,547,652 (2003).
90. E.C. Wilson, H.A. Anderson, G. Appel, US Patent 6,149,512 (2000).
91. Internet web site: http://www.lamrc.com, © Lam Research Inc., 2001.
92. N. Shendon, US Patent 5,899,800 (1999).
93. N. Shendon, D.R. Smith, Patent 5,582,534 (1996).
94. Characterization and optimization of copper chemical–mechanical planarization10.1007/s11664-002-0043-5 ↗
95. L.P. Lai, J.L. Tucker, R.J. Lujan, US Patent 6,224,472 (2001).
96. Internet web site: http://www.nikon.co.jp/main/eng/products/cmp_e.htm, Nikon Corporation, 2003.
97. Infenion Corporation, http://www.infenion.com/, © Infenion Corporation, 2003.
98. Sensys instruments, wafer-to-wafer control of advanced dual damascene W CMP processes for volume production
99. The theory and design of plate glass polishing machines
100. Investigating slurry transport beneath a wafer during chemical mechanical polishing processes10.1149/1.1393455 ↗