Properties of lead-free solder alloys with rare earth element additions
Source abstract
Abstract
Abstract Due to the inherent toxicity of lead (Pb), environmental regulations around the world have been targeted to eliminate the usage of Pb-bearing solders in electronic assemblies. This has prompted the development of “Pb-free” solders, and has enhanced the research activities in this field. In order to become a successful solder material, Pb-free alloys need to be reliable over long term use. Although many of these alloys possess higher strength than the traditional Sn–Pb ones, there still exist reliability problems such as electromigration and creep. Also, the solderability of many Pb-free alloys is inferior to that of Sn–Pb and any improvement or replacement will be welcomed by industry. In order to develop new Pb-free solders with better properties, trace amounts of rare earth (RE) elements were selected by some researchers as alloying additions into Sn-based solders. These solder alloys are mainly Sn–Ag, Sn–Cu, Sn–Zn and Sn–Ag–Cu. In general, the resulting RE-doped solders are found to have better performances than their original ones. The improvements include better wettability, creep strength and tensile strength. In particular, the increase in creep resistance in some RE-doped alloys gives creep rupture time increases by over four times for Sn–Ag and seven times for Sn–Cu and Sn–Ag–Cu. Like other Sn-based alloys, their creep rates are controlled by dislocation pipe diffusion in the Sn matrix. Also, it was found that the creep rate of these Sn-based alloys can be represented by a single empirical equation. With the addition of RE elements, solders for bonding on difficult substrates such as on semiconductors, diamond, and optical materials have also been developed. This report summarizes the effect of RE elements on the microstructure, mechanical properties, wetting behavior of certain Pb-free solder alloys. As an illustration of the advantage of RE doping, interfacial studies were carried out for electronic interconnections with RE-doped Pb-free alloys. It was found that the intermetallic compound (IMC) layer thickness and the amount of interfacial reaction were reduced in a Ball Grid Array (BGA) package. These results indicate that RE elements would play an important role in providing better electronic interconnections.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Tin–lead (Sn–Pb) solder reaction in flip chip technology10.1016/S0927-796X(01)00029-8 ↗
2. In search of new lead-free electronic solders10.1007/BF02651363 ↗
3. ASM International, Electronic Material Handbook, vol. 1, Materials Park, OH, 1989, pp. 965–966.
4. Global update on lead-free solders
5. J. Cannis, Green IC packaging, Adv. Packaging (8) (2001) 33–38.
6. International Printed Circuit Association Solder Products Value Council, White Paper: IPC-SPVC-WP-006 Round Robin Testing and Analysis, Lead Free Alloys: Tin, Silver, Copper, 12 August 2003.
7. Lead-free solders in microelectronics10.1016/S0927-796X(00)00010-3 ↗
8. Developing a lead-free solder alloy Sn–Bi–Ag–Cu by mechanical alloying10.1007/s11664-000-0166-5 ↗
9. Advances in lead-free electronics soldering10.1016/S1359-0286(00)00036-X ↗
10. Alloying effects in near-eutectic Sn–Ag–Cu solder alloys for improved microstructural stability10.1007/s11664-001-0129-5 ↗
11. New Pb-free solder alloy with superior mechanical properties10.1063/1.109734 ↗
12. Lead-free alloys10.1108/09540919810203793 ↗
13. Thermodynamic database for phase diagrams in micro-soldering alloys10.1007/s11664-999-0152-5 ↗
14. Thermodynamic calculation of the In–Sn–Zn ternary system10.1016/S0925-8388(00)01484-5 ↗
15. Experimental determination and thermodynamic calculation of the phase equilibria and surface tension in the Sn–Ag–In system10.1007/s11664-002-0003-0 ↗
16. How $1-billion per year can be saved in the soldering of electronic compounds
17. Hard-particle reinforced composite solders. Part 1. Microcharacterisation10.1108/09540919710800647 ↗
18. Metallurgical changes in tin–lead platings due to heat aging10.1109/33.105118 ↗
19. Processing dispersion-strengthened Sn–Pb solders to achieve microstructural refinement and stability10.1016/0956-716X(91)90023-T ↗
20. D.L. Deborah Chung, Carbon fiber reinforced tin–lead alloy as a low thermal expansion solder perform, US Patent 5,089,356 (1992).
21. Dispersed additions to a Pb-free solder for suppression of microstructural coarsening10.1007/BF02651367 ↗
22. A viable tin–lead solder substitute: Sn–Ag–Cu10.1007/BF02653344 ↗
23. Reflow characteristics of Sn–Ag matrix in-situ composite solders10.1016/S1359-6462(99)00392-9 ↗
24. Microstructure of a lead-free composite solder produced by an in-situ process10.1007/s11664-002-0024-8 ↗
25. Microstructural engineering of solders10.1007/s11664-999-0154-3 ↗
26. Conception of a consumable copper reaction zone for a NiTi/SnAgCu composite material10.1016/S1359-835X(02)00154-9 ↗
27. Z.G. Yu, M.B. Chen, Rare Earth Elements and their Applications, Metallurgical Industry Press, 1995, 138-273.
28. Microstructure and mechanical properties of Pb-free solder alloys for low cost electronic assembly: a review10.1007/BF02651361 ↗
29. The properties of Sn–9Zn lead-free solder alloys doped with trace rare earth elements10.1007/s11664-002-0184-6 ↗
30. Improvements of microstructure, wettability, tensile and creep strength of eutectic Sn–Ag alloy by doping with rare earth elements10.1557/JMR.2002.0455 ↗
31. Wetting and interface microstructure between Sn–Zn binary alloys and Cu10.1557/JMR.1998.0391 ↗
32. Microstructure and mechanical properties of new lead-free Sn–Cu–RE solder alloys10.1007/s11664-002-0185-5 ↗
33. Ueber den Auf-bau des Systems Silber-Kupfer-Zinn
34. Tin–silver–copper eutectic temperature and composition10.1007/s11661-000-0111-5 ↗
35. Experimental and thermodynamic assessment of Sn–Ag–Cu solder alloys10.1007/s11664-000-0003-x ↗
36. Determination of the eutectic structure in the Ag–Cu–Sn system10.1007/s11664-002-0163-y ↗
37. Effects of cooling speed on microstructure and tensile properties of Sn–Ag–Cu alloys10.1016/S0921-5093(01)01828-7 ↗
38. Interaction relation in 60Sn–Pb–0.05La ternary solder alloy10.1016/S0167-577X(02)00521-9 ↗
39. The wettability and microstructure of Sn–Zn–RE alloys10.1007/s11664-003-0238-4 ↗
40. Effect of rare earth element additions on the microstructure and mechanical properties of tin–silver–bismuth solder10.1007/s11664-002-0126-3 ↗
41. Study on the microstructure of a novel lead-free solder alloy SnAgCu–RE and its soldered joints10.1007/s11664-002-0052-4 ↗
42. Properties of lead-free solder SnAgCu containing minute amounts of rare earth10.1007/s11664-003-0215-y ↗
43. H. Baker, et al. (Eds.), Alloy phase diagrams, ASM Handbook 3, Materials Park, OH, 1990, p. 137.
44. H. Baker, et al. (Eds.), Alloy phase diagrams, ASM Handbook 3, Materials Park, OH, 1990, p. 275.
45. Universal solders for direct and powerful bonding on semiconductors, diamond, and optical materials10.1063/1.1370985 ↗
46. Q.J. Zhai, S.K. Guan, Q.Y. Shang, Alloy Thermo-Mechanism: Theory and Application, Metallurgy Industry Press, Beijing, 1999.
47. The creep properties of precipitation-strengthened tin-based alloys10.1007/s11837-000-0146-5 ↗
48. Microstructure changes in Sn–3.5Ag solder alloy during creep10.1007/s11664-998-0099-y ↗
49. Creep phenomena in lead-free solders10.1007/s11664-000-0150-0 ↗
50. Fracture of Sn–3.5(percent)Ag solder alloy under creep10.1007/s11664-000-0119-z ↗
51. Creep behavior of eutectic Sn–Ag lead-free solder alloy10.1557/JMR.2002.0420 ↗
52. High temperature deformation of oxide dispersion strengthened Al and Al–Mg solid solution10.1016/0001-6160(82)90153-5 ↗
53. Creep behavior of eutectic Sn–Cu lead-free solder alloy10.1007/s11664-002-0098-3 ↗
54. Effect of substrate preheating on solderability performance as a guideline for assembly process development. Part 1. Baseline analysis10.1108/09540919610777708 ↗
55. Wettability test method for surface mount technology assessment10.1108/09540910010331329 ↗
56. Issues in the replacement of lead-bearing solders10.1007/BF03222374 ↗
57. C.M.T. Law, C.M.L. Wu, D.Q. Yu, M. Li, Solderability and growth of intermetallic compounds upon aging of Sn–Ag–RE and Sn–Cu–RE lead-free alloys, Presented at Conference of Material Science & Technology 2003, 9–11 November 2003, Chicago.
58. C.M.L. Wu, C.M.T. Law, D.Q. Yu, L. Wang, unpublished wettability results.
59. New lead-free, Sn–Zn-In solder alloys10.1007/BF02653357 ↗
60. P. Nash, A. Nash, H. Baker, et al. (Eds.), Alloy phase diagrams, ASM Handbook 3, Materials Park, OH, 1990, p. 32 (Section 2).
61. IPC, IPC Roadmap on Lead-free Soldering, 3rd draft, 2003.
62. The mechanical behavior of interconnect materials for electronic packaging10.1007/BF03222944 ↗
63. Effect of interface roughness on fatigue crack growth in Sn–Pb solder joints10.1115/1.2792148 ↗
64. Spalling of Cu6Sn5 spheroids in the soldering reaction of eutectic SnPb on Cr/Cu/Au thin films10.1063/1.363728 ↗
65. Three-dimensional morphology of a very rough interface formed in the soldering reaction between eutectic SnPb and Cu10.1063/1.113975 ↗
66. Kinetic analysis of the soldering reaction between eutectic SnPb alloy and Cu accompanied by ripening10.1103/PhysRevB.53.16027 ↗
67. The formation and growth of intermetallic in composite solder10.1007/BF02817353 ↗
68. Intermetallic phase formation in thin solid–liquid diffusion couples10.1007/BF02651374 ↗
69. Characterizing the formation and growth of intermetallic compound in the solder joint10.1023/A:1004499728840 ↗
70. Intermetallic compound layer formation between copper and hot-dipped 100In, 50In–50Sn, 100Sn, and 63Sn–37Pb coatings10.1007/BF02653343 ↗
71. Effect of soldering and aging time on interfacial microstructure and growth of intermetallic compounds between Sn–3.5Ag solder alloy and Cu substrate10.1007/s11664-000-0014-7 ↗
72. An improved numerical method for predicting intermetallic layer thickness developed during the formation of solder joints on Cu substrate10.1007/s11664-999-0157-0 ↗
73. D.Q. Yu, C.M.L. Wu, C.M.T. Law, L. Wang, Intermetallic compounds growth between Sn–3.5Ag lead-free solder and Cu substrate during soldering and aging, submitted for publication.
74. Wetting reaction versus solid state aging of eutectic SnPb on Cu10.1063/1.1357469 ↗
75. Morphology, kinetics, and thermodynamics of solid-state aging of eutectic SnPb and Pb-free solders (Sn–3.5 Ag, Sn-3.8 Ag–0.7 Cu and Sn–0.7 Cu) on Cu10.1557/JMR.2002.0042 ↗
76. Physics and materials challenges for lead-free solders10.1063/1.1517165 ↗
77. Scallop formation and dissolution of Cu–Sn intermetallic compound during solder reflow10.1063/1.1445283 ↗
78. Interface reaction between copper and molten tin–lead solders10.1016/S1359-6454(01)00146-X ↗
79. Dependence of Cu/Sn and Cu/60Sn40Pb solder joint strength on diffusion controlled growth of Cu3Sn and Cu6Sn510.1557/PROC-40-129 ↗
80. Effect of La on the Cu–Sn intermetallic compound (IMC) growth and solder joint reliability10.1016/S0925-8388(01)01747-9 ↗
81. Activation energies of intermetallic growth of Sn–Ag eutectic solder on copper substrates10.1007/s11664-997-0268-4 ↗
82. Characterization of the growth of intermetallic interfacial layers of Sn–Ag and Sn–Pb eutectic solders and their composite solders on Cu substrate during isothermal long-term aging10.1007/s11664-999-0159-y ↗
83. Kinetics of interfacial reaction in bimetallic Cu–Sn thin films10.1016/0001-6160(82)90201-2 ↗
84. Irreversible processes of spontaneous whisker growth in bimetallic Cu–Sn thin-film reactions10.1103/PhysRevB.49.2030 ↗
85. Solder reaction-assisted crystallization of electroless Ni-P under bump metallization in low cost flip chip technology10.1063/1.370627 ↗
86. Y.-D. Jeon, K.-W. Paik, K.-S. Bok, W.-S. Choi, C.-L. Cho, Studies on Ni–Sn intermetallic compound and P-rich Ni layer at the electroless nickel UBM–solder interface and their effects on flip chip solder joint reliability, in: Proceedings of the 51th Electronic Components & Technology Conference, 29 May–31 June 2001, Orlando, FL, IEEE, Piscataway, USA, 2001, pp. 1326–1332.
87. The reactions between electroless Ni–Cu–P deposit and 63Sn–37Pb flip chip solder bumps during reflow10.1007/s11664-000-0165-6 ↗
88. Correlation between Ni3Sn4 intermetallics and Ni3P due to solder reaction-assisted crystallization of electroless Ni–P metallization in advanced packages10.1557/JMR.2000.0363 ↗
89. Study of Ni3P growth due to solder reaction-assisted crystallization of electroless Ni–P metallization10.1023/A:1006735103744 ↗
90. Thermal stability of electroless-Ni/solder interfaces. Part A. Interfacial chemistry and microstructure10.1007/BF02830353 ↗
91. V. Vuorinen, K. Zeng, J.K. Kivilahti, A TEM study of interfacial reaction in SnAgCu solder joints on the Ni(P) coated PCBs, in press.
92. K. Zeng, V. Vuorinen, J. K. Kivilahti, Intermetallic reactions between lead-free SnAgCu solder and Ni(P)/Au surface finish on PWBs, in: Proceedings of the 51th Electronic Components & Technology Conference, 29 May–31 June 2001, Orlando, FL, IEEE, Piscataway, USA, 2001, pp. 685–690.10.1109/ECTC.2001.927808 ↗
93. K. Zeng, V. Vuorinen, J. K. Kivilahti, Interfacial reactions between lead-free SnAgCu solder and Ni(P) surface finish on PWBs, IEEE Trans. CPMT, submitted for publication.
94. C.M.T. Law, C.M.L. Wu, D.Q. Yu, M. Li, D.Z. Chi, Interfacial microstructure evolution of lead-free Sn–Zn–RE solder balls on BGA packages, J. Mater. Res., submitted for publication.
95. C.M.T. Law, C.M.L. Wu, D.Q. Yu, M. Li, D.Z. Chi, Microstructure Evolution of Lead-free Sn–Zn, and Sn–Zn–RE BGA solder bumps, submitted for publication.
96. The growth of intermetallic compounds at Sn–Ag–Cu Solder/Cu and Sn–Ag–Cu solder/Ni interfaces and the associated evolution of the solder microstructure10.1007/s11664-001-0144-6 ↗
97. Effect of Cu concentration on the interfacial reactions between Ni and Sn–Cu solders10.1557/JMR.2002.0036 ↗
98. Effect of Cu concentration on the reactions between Sn–Ag–Cu solders and Ni10.1007/s11664-002-0129-0 ↗
99. Lead-free universal solders for optical and electronic devices10.1007/s11664-002-0005-y ↗
100. Bonding nature of rare-earth-containing lead-free solders10.1063/1.1435075 ↗