journal article·2021-01-01Open access

Transient liquid phase bonding of silicon and direct bond copper via electroplating of tin-copper interlayers for power device applications

Hyejun Kang, Ashutosh Sharma, Jung-Hyun Lee, Jae Pil Jung

Materials Research Express· Volume 8· Issue 1

Abstract

Abstract Joining technology of silicon semiconductors devices to direct bond copper (DBC) substrates in high-temperature power electronics packages is of utmost importance today. In this study, Sn–Cu solder was prepared by electroplating on a direct bonded copper (DBC) substrate. The electroplated DBC system thus prepared was TLP bonded with Si chip at 250 °C for 10 min under a vacuum atmosphere. The effect of electrical charge used for plating Sn–Cu solder, void fraction in the joint, Sn–Cu solder composition on the joining characteristics, and shear strength of the Si-DBC system were analyzed. The experimental results showed that the plating thickness increased almost linearly with plating time and electrical charge. A sound Sn–Cu solder plating thickness was obtained at 40 mA cm−2, 11 C cm−2, 20 min with 20 at% Cu in the deposit. Furthermore, the plated Sn–Cu solder layer transformed to Cu6Sn5 and Cu3Sn after joining at 250 °C for 10 min. The shear bonding strength of the Si/DBC joint increased with Cu content in the Sn–Cu solder until 20 at% in the Sn–Cu interlayer.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Status and trend of power semiconductor module packaging for electric vehicles10.5772/64173 ↗
2. Overview of transient liquid phase and partial transient liquid phase bonding10.1007/s10853-011-5561-1 ↗
3. A review: formation of voids in solder joint during the transient liquid phase bonding process—Causes and solutions10.1016/j.microrel.2019.04.024 ↗
4. Advances in lead-free electronics soldering10.1016/S1359-0286(00)00036-X ↗
5. A high temperature, double-sided cooling SiC power electronics module10.1109/ECCE.2013.6647075 ↗
6. Pulse electrodeposition of lead-free tin-based composites for microelectronic packaging10.5772/62036 ↗
7. Lifetime prediction of solders in electronic packaging
8. Creep deformation behavior in eutectic Sn–Ag solder joints using a novel mapping technique10.1007/s11664-999-0167-y ↗
9. Interfacial reactions between lead-free solders and common base materials10.1016/j.mser.2005.03.001 ↗
10. Characterization of plate-like Ni-Sn intermetallic compounds in Sn–Ag solder bump10.1109/IPFA.2017.8060200 ↗
11. Nanoparticle/solder hybrid joints for next-generation power semiconductor modules10.1016/j.matdes.2017.03.061 ↗
12. Properties and microstructures of Sn–Ag–Cu–X lead-free solder joints in electronic packaging10.1155/2015/639028 ↗
13. Study on low melting nanocrystalline Sn–0.7Cu solder alloy10.4314/ijest.v10i3.2 ↗
14. Properties and microstructures of Sn–Bi-X lead-free solders10.1155/2016/9265195 ↗
15. Mechanical properties of Sn–Zn lead-free solder alloys based on the microstructure array10.1016/j.matchar.2009.11.012 ↗
16. The Effect of epoxy polymer addition in Sn–Ag–Cu and Sn–Bi solder joints10.3390/ma12060960 ↗
17. Research advances in nano-composite solders10.1016/j.microrel.2008.10.004 ↗
18. Microstructure and brazeability of SiC nanoparticles reinforced Al–9Si–20Cu produced by induction melting10.1179/1743284715Y.0000000138 ↗
19. Synthesis of Sn–Ag binary alloy powders by mechanical alloying10.1016/j.matchemphys.2010.02.075 ↗
20. Electroplating and electroless plating10.1016/B978-0-08-096532-1.00413-1 ↗
21. Paunovic · 200610.1002/0470009403 ↗
22. Pulse plated Sn–Cu solder coatings from stannate bath10.1108/SSMT-08-2019-0027 ↗
23. The effect of electrical charge density on the transition behavior between bonding and clogging stages of an electroplated porous surface10.1016/j.jmatprotec.2019.03.009 ↗
24. The effect of current density on the grain size of electrodeposited nanocrystalline nickel coatings10.1016/j.surfcoat.2008.01.018 ↗
25. The effect of plating current densities on self-annealing behaviors of electroplated copper films10.1149/1.1500348 ↗
26. Impurity and alloying effects on interfacial reaction layers in Pb-free soldering10.1016/j.mser.2009.12.001 ↗
27. A study of intermetallic compound formation in a copper-tin bimetallic couple10.1063/1.345324 ↗
28. Preferred orientation relationship between Cu6Sn5 scallop-type grains and Cu substrate in reactions between molten Sn-based solders and Cu10.1063/1.2776002 ↗
29. Interfacial diffusion of copper in tin10.1063/1.1710127 ↗
30. Intermetallic growth and Kirkendall effect manifestations in Cu/Sn and Au/Sn diffusion couples10.3139/146.018032 ↗
31. Segregant-induced cavitation of Sn/Cu reactive interface10.1016/j.scriptamat.2005.05.033 ↗
32. A comparative study of Cn/Sn/Cu and Ni/Sn/Ni solder joints for low temperature stable transient liquid phase bonding10.1016/j.scriptamat.2015.07.032 ↗